Chemically coupled hydroxyapatite-polyethylene composites: structure and properties.

Silanation of hydroxyapatite and acrylic acid grafting of polyethylene were employed to improve bonding between hydroxyapatite and polyethylene. The structure and properties of chemically coupled hydroxyapatite reinforced high-density polyethylene (HA/HDPE) composites were subsequently investigated using various techniques. It was shown that there existed a silicon-containing interphase between the hydroxyapatite particle and the polyethylene matrix. The silane coupling agent used promoted chemical adhesion between hydroxyapatite particles and the polymer. The use of the silane coupling agent also facilitated the penetration of polymer into cavities in individual ceramic particles, which resulted in enhanced mechanical interlocking at the matrix-reinforcement interface. With a strong bond (both mechanical and chemical) being formed between hydroxyapatite and polyethylene, chemically coupled HA/HDPE composites possessed improved mechanical properties and fracture behaviour.

Durapatite↗

Initial interaction of osteoblasts with the surface of a hydroxyapatite-poly(methylmethacrylate) cement.

Failure of the bone/cement interface in cemented joint prostheses is a contributor to implant loosening. The introduction of a bioactive phase, such as hydroxyapatite (HA), to cement may enhance fixation by encouraging direct bone apposition rather than encapsulation of the implant by fibrous tissue. The effect of poly(methylmethacrylate) (PMMA) bone cement (incorporating 17.5% HA wt.) on bioactivity has been investigated using primary human osteoblast-like cells (HOB). A significantly higher cell proliferation and differentiation was seen on the PMMA/HA cement compared to the PMMA cement alone, with retention of phenotype up to 21 days of culture on both materials.

Bone Cements↗

Fatigue of cortical bone under combined axial-torsional loading.

The influence of torsional loading on the fatigue life of cortical bone was investigated by conducting in vitro testing. Fatigue tests were conducted on cylindrical dumbbell bovine cortical bone specimens in an environmental chamber under axial loading, torsional loading and various combinations of axial-torsional loading where the phase relationship and relative magnitudes of axial and torsional loadings were systematically varied. It was found that the superposition of torque on axial loading reduced the fatigue life of cortical bone. The reduction in fatigue life was significant when the maximum shear stress was greater than 59% of the maximum normal stress. The magnitude of reduction in the fatigue life of bone at low as well as high levels of axial loading depended on the magnitude of torsional loading, but was independent of the phase angle by which the torsional loading lagged the axial loading. Furthermore, oblique fracture profiles, characteristic of torsion-induced failure, were observed for combined axial-torsional load cases. Based on these results, it is suggested that torsional loading plays a significant role in determining the fatigue life of cortical bone.

Animals↗

Effect of powder characteristics on the sinterability of hydroxyapatite powders.

The effect of different sintering conditions on the sintered density and microstructure of two different hydroxyapatite (HA) powders was examined. The powder characteristics of a laboratory synthesized HA powder (Lab HA) were low crystallinity, a bimodal particle size distribution, a median particle size of 22 microm and a high specific surface area (SSA) of 63 m2/g. By contrast, a commercial calcined HA (commercial HA) was crystalline and had a median particle size of 5 microm and a low SSA of 16 m2/g. The different powder characteristics affected the compactability and the sinterability of the two HA powders. Lab HA did not compact as efficiently as commercial HA, resulting in a lower green density, but the onset of sintering of powder compacts of the former was approximately 150 degrees C lower than the later. The effect of compaction pressure, sintering temperature, time and heating rate on the sintered densities of the two materials was studied. Varying all these sintering conditions significantly affected the sintered density of commercial HA, whereas the sintered density of Lab HA was only affected significantly by increasing the sintering temperature. The Vickers hardness, Hv, of Lab HA was greater than commercial HA for low sintering temperatures, below 1200 degrees C, whereas for higher sintering temperatures the commercial HA produced ceramics with greater values of hardness. These trends can be related to the sinterability of the two materials.

Journal Article↗

Calcining influence on the powder properties of hydroxyapatite.

The effect of different calcination temperatures on the powder characteristics and the sintered density of synthetic hydroxyapatite (HA) powders, produced using two different processing routes, was examined. Powders were produced by either drying, milling and sieving an as-precipitated HA or by spray-drying a slurry of precipitated HA. Calcining the two powders at temperatures between 400 and 1000 degrees C did not significantly affect the powder particle size. The specific surface areas of the two powders, however, were reduced from 70-80 m2/g for a calcination temperature of 400 degrees C to approximately 5-7 m2/g for 1000 degrees C. Analysis of the surfaces of the HA powders using scanning electron microscopy (SEM) illustrated the coarsening and subsequent sintering of the sub-micron crystallites that constitute a powder particle as the calcination temperature increased, corresponding to the decrease in surface area of the powders. The sintered densities of the final ceramics were not significantly affected by calcining the powders. Microhardness measurements of ceramics prepared from powders calcined at different temperatures showed no significant variations with calcination temperature or powder processing method. The results of this study have illustrated that for applications where HA may be used in powder form, for example in plasma-spraying and for the production of HA-polymer composites, calcining the HA will significantly affect the powder properties, namely the surface area and morphology of the powders. For applications requiring HA in a dense ceramic form, for example as granules or blocks, calcining the powders does not significantly affect the properties of the final ceramic.

Journal Article↗

Fatigue characterization of a hydroxyapatite-reinforced polyethylene composite. I. Uniaxial fatigue.

The fatigue behavior of 40 volume % hydroxyapatite-reinforced polyethylene composite (HAPEXtrade mark) at 37 degrees C in saline was determined. S-N curves for this material, both in fully reversed axial tension-compression and fully reversed torsion, have been established. In tension, the cycles to failure ranged from 1000 cycles at 13 MPa to more than 1 million cycles at 4.4 MPa while in torsion they ranged from 100 cycles at 14.4 MPa to more than 1 million cycles at 4.8 MPa. Changes in strain range, tangent modulus, and cyclic energy dissipated during fatigue loading also were examined. Torsional fatigue was found to be considerably more damaging than axial fatigue. The fatigue damage accumulation process occurring in the composite was monitored by observing the reduction in modulus and the increase in energy dissipated.

Biocompatible Materials↗

Fatigue characterization of a hydroxyapatite-reinforced polyethylene composite. II. Biaxial fatigue.

Previously, the uniaxial fatigue behavior of 40 volume % hydroxyapatite-reinforced polyethylene composite (HAPEXtrade mark) at 37 degrees C in saline was studied. Fatigue limits between 37 and 25% of the ultimate strengths of the material were established. This study investigates the biaxial fatigue behavior of the same material using various combinations of axial and torsional stresses. The addition of torsional to axial loading significantly reduced the fatigue life. When torsion at 25% of the ultimate strength was applied in addition to axial loading at 25% of the ultimate tensile strength, the fatigue life remained more than 1 million cycles. Out-of-phase loading was less detrimental to the fatigue life of the composite than in-phase. Fatigue damage was monitored by hysteresis loops, the increase in dissipated energy, the reduction in tangent modulus, and the increase in strain values.

Biocompatible Materials↗

Analysis of apatite layers on glass-ceramic particulate using FTIR and FT-Raman spectroscopy.

A nucleation and crystallization schedule was adapted to produce 40% crystalline Bioglass ceramic particulates. These particles were placed in a dynamic environment in a simulated physiologic solution (SBF-9) for time periods ranging from 10 min to 7 days. Fourier transform Raman spectroscopy (FT-Raman) and infrared spectroscopy (FTIR) were used to analyze the apatite layer formation on the particulates. FTIR determined that amorphous apatite formation took place within 2 h, with the appearance of crystalline apatite in 14 h. The vibrational frequencies obtained through FT-Raman were equivalent to those obtained using FTIR. These analyses showed that a fully crystallized apatite layer was present on the particulate after 3 days of exposure in SBF solution. These findings are consistent with those associated with amorphous Bioglass particles.

Apatites↗

Tensile characteristics of ten commercial acrylic bone cements.

The mechanical properties of acrylic bone cement, used in orthopedic surgery, are very influential in determining successful long-term stability of a prosthesis. A large number of commercial formulations are available, differing in chemical composition and physical properties of both powder and monomer constituents. In this study, the static and dynamic tensile characteristics of a number of the most commonly used bone cements (Palacos R, Simplex P, CMW 1 & 3, Sulfix-60, Zimmer Dough), along with some newer formulations (Endurance, Duracem 3, Osteobondtrade mark and Boneloc), have been investigated under the same testing regimes. Testing was performed in air at room temperature. Significant differences in both static and fatigue properties were found between the various bone cements. Tensile tests revealed that Palacos R, Sulfix-60, and Simplex P had the highest values of ultimate tensile strength, closely followed by CMW 3, while Zimmer Dough cement had the lowest strength. Fatigue testing was performed under stress control, using sinusoidal loading in tension-tension, with an upper stress level of 22MPa. The two outstanding cements when tested in these cyclic conditions were Simplex P and Palacos R, with the highest values of Weibull median cycles to failure. Boneloc bone cement demonstrated the lowest cycles to failure. While the testing regimes were not designed to replicate exact conditions experienced by the bone cement mantle in vivo, there was a correlation between these results and clinical outcome.

Bone Cements↗

Contribution, development and morphology of microcracking in cortical bone during crack propagation.

A fracture mechanics study of cortical bone is presented to investigate the contribution, development morphology of microcracking in cortical bone during crack propagation. Post-hoc analyses of microcrack orientation, crack propagation velocity and fracture surface roughness were conducted on previously tested human and bovine bone compact tension specimens. It was found that, consistent with its higher toughness, bovine bone formed significantly more longitudinal, transverse and inclined microcracks than human bone. However, in human bone more of the microcracks that formed were longitudinal than transverse or inclined, a feature that would optimise bone's toughness. Crack propagation velocity in human and bovine bone displayed the same characteristic pattern with crack extension, where an increase in velocity is followed by a consequent decrease and vice versa. On the basis of this pattern, a model or crack propagation has been proposed. It provides a detailed account of mocrocrack formation and contribution towards the propagation of a fracture crack. Analyses of fracture surfaces indicated that, consistent with its higher toughness, bovine bone displays a rougher surface than human bone but they both have the same basic fractured element, i.e. a mineralised collagen fibril.

Animals↗

Characterization of the transformation from calcium-deficient apatite to beta-tricalcium phosphate.

The structural changes that occur during the transformation of a Ca-deficient apatite, prepared by a wet chemical method, to beta-TCp were investigated. X-ray diffraction (XRD) analysis of as-prepared samples and samples calcined at temperatures between 500 and 1100 degrees C showed that the transformation occurs over the temperature range 710-740 degrees C, under non-equilibrium conditions. The change in crystallite size with increasing calcination/sintering temperature was studied by XRD using the Scherrer formula. Fourier transform infra-red (FTIR) analysis indicated considerable structural change in samples above and below this temperature range. Changes were observed in the hydroxyl, carbonate and phosphate bands as the calcination temperature was increased from 500 to 1100 degrees C. Even once a single beta-TCP phase is obtained at 740 degrees C there remains a considerable amount of structural change at temperatures between 740 and 1100 degrees C. This effect was illustrated by an unusual change in the lattice parameters of the beta-TCP structure and significant changes in the phosphate bands of FTIR spectra as the calcination temperature was increased. The results obtained in this study show that the combined experimental techniques of XRD and FTIR are excellent complimentary methods for characterizing structural changes that occur during phase transformations.

Journal Article↗

Bone fracture analysis on the short rod chevron-notch specimens using the X-ray computer micro-tomography.

Mechanical fatigue of bone leads to micro-cracking which is associated with remodeling, establishing a balance in the microcrack population of the living tissue, thus, in the steady-state, the microstructure of bone provides sites of discontinuity acting as stress raisers. Hence fracture toughness plays a decisive role in bone functionality by determining the level to which the material can be stressed in the presence of cracks, or, equivalently, the magnitude of cracking which can be tolerated at a given stress level. Cortical bone, which behaves as a quasi-brittle solid when fractured, was tested as short-rod chevron-notched tension specimens (CNT). The main features of the CNT specimen are its geometry and the V shaped notch. The notch leads to steady-state crack propagation whilst the requested geometry allows a diameter 40% smaller than the thickness of a standard compact tension specimens (CT). These features are essential to distinguish the inhomogeneties in the fracture properties of materials like bone. Bone structure and crack propagation of the CNT specimens were analyzed using X-ray computed micro-tomography (XMT), which is a non-invasive imaging technique. The unique feature of the micro-CT is the high resolution three-dimensional image which consists of multi-sliced tomographs taken in a fine pitch along the rotational axis. Fracture toughness (K(IC)) computed according to the peak load was 4.8 MNm(-3/2) while that derived from experimental calibration tests using XMT was 4.9 MNm(-3/2).

Journal Article↗

Surface topography and HA filler volume effect on primary human osteoblasts in vitro.

HAPEX, a bone analog material, with similar properties to cortical bone, has been studied in vitro with particular reference to the effect of surface topography. The stimulation of a favorable bone response by this composite depends on optimization of the hydroxyapatite (HA) content in relation to the material bioactivity without compromising the mechanical characteristics. In this study we have started to investigate the effects of surface topography on cell attachment and subsequent cellular behavior in relation to proliferation. Different volumes of HA (20% and 40%) were added to a high density polyethylene (HDPE) matrix to produce the test materials. Scanning electron microscopy (SEM) and confocal laser scanning microscopy (CLSM) were used to examine cell morphology on HAPEX, and the surface characteristics produced by different machining protocols. The measurement of cellular DNA and tritiated thymidine ([3H]-TdR) incorporation has been used to asses cell proliferation upon the materials. The results show that the material surface topography has a large influence on cell proliferation and attachment, and with a controlled material topography the 40% vol HA/HDPE composite gives the greater biological response compared to the 20% vol HA/HDPE composite.

Journal Article↗

Dynamic mechanical characterization of hydroxyapatite reinforced polyethylene: effect of particle size.

Dynamic mechanical analysis (DMA) was used to characterize biomedical composites consisting of synthetic hydroxyapatite (HA) particulate reinforced polyethylene (PE). The effects of the HA volume fraction, temperature and HA particle on the storage modulus (E(I)) and damping (tan delta) were investigated. Increasing HA volume fractions increased E(I) and decreased tan delta. E(I) was found to be linearly related to the Young's modulus values obtained from quasi-static tensile tests. Relative modulus and damping studies showed that the viscoelastic behavior of unfilled PE was different to that of the filled matrix due to the presence of thermally induced tensile stresses in the matrix at the filler-matrix interface.

Journal Article↗

Characterization of the transformation from calcium-deficient apatite to beta-tricalcium phosphate.

The structural changes that occur during the transformation of a Ca-deficient apatite, prepared by a wet chemical method, to beta-TCP were investigated. X-ray diffraction (XRD) analysis of as-prepared samples and samples calcined at temperatures between 500 and 1100 degrees C showed that the transformation occurs over the temperature range 710-740 degrees C, under non-equilibrium conditions. The change in crystallite size with increasing calcination/sintering temperature was studied by XRD using the Scherrer formula. Fourier transform infra-red (FTIR) analysis indicated considerable structural change in samples above and below this temperature range. Changes were observed in the hydroxyl, carbonate and phosphate bands as the calcination temperature was increased from 500 to 1100 degrees C. Even once a single beta-TCP phase is obtained at 740 degrees C there remains a considerable amount of structural change at temperatures between 740 and 1100 degrees C. This effect was illustrated by an unusual change in the lattice parameters of the beta-TCP structure and significant changes in the phosphate bands of the FTIR spectra as the calcination temperature was increased. The results obtained in this study show that the combined experimental techniques of XRD and FTIR are excellent complimentary methods for characterizing structural changes that occur during phase transformations.

Journal Article↗

Effect of sintering parameters on the density and microstructure of carbonate hydroxyapatite.

This work documents an investigation into the effect of water on the density and microstructure of carbonate hydroxyapatite in carbon dioxide sintering atmospheres. Carbonate apatites with carbonate contents of between 3.2 and 7.8 wt % were precipitated and the precipitates were formed into dry gels. Isothermal and isochronal sintering experiments were performed under dry carbon dioxide and wet carbon dioxide (containing 3 wt % water) atmospheres. The effect of carbonate content was studied by using two gels both with a green density of 37% and with carbonate contents of 5.8 and 7.8 wt %. Both isothermal and isochronal experiments demonstrated that bloating of the apatite occurred and this behavior was associated with the loss of carbonate from the apatite. It was found that only in wet carbon dioxide atmospheres fully dense translucent carbonate apatite could be formed. 93% dense carbonate apatite was formed after 4 h sintering at temperatures as low as 700 degrees C.

Journal Article↗

Stress transmission through Ti-Ni alloy, titanium and stainless steel in impact compression test.

Impact stress transmission of Ti-Ni alloy was evaluated for biomedical stress shielding. Transformation temperatures of the alloy were investigated by means of DSC. An impact compression test was carried out with use of split-Hopkinson pressure-bar technique with cylindrical specimens of Ti-Ni alloy, titanium and stainless steel. As a result, the transmitted pulse through Ti-Ni alloy was considerably depressed as compared with those through titanium and stainless steel. The initial stress reduction was large through Ti-Ni alloy and titanium, but the stress reduction through Ti-Ni alloy was more continuous than titanium. The maximum value in the stress difference between incident and transmitted pulses through Ti-Ni alloy or titanium was higher than that through stainless steel, while the stress reduction in the maximum stress through Ti-Ni alloy was statistically larger than that through titanium or stainless steel. Ti-Ni alloy transmitted less impact stress than titanium or stainless steel, which suggested that the loading stress to adjacent tissues could be decreased with use of Ti-Ni alloy as a component material in an implant system.

Journal Article↗

Mechanical properties of hydroxyapatite reinforced poly(ethylmethacrylate) bone cement after immersion in a physiological solution: influence of a silane coupling agent.

PEMA-based bone cement has previously been shown to possess many advantages over traditional PMMA cements. One of these is the option of adding up to 40 wt % HA without a decrease in static mechanical strength, thus providing the potential for enhanced bioactivity. Bone cement, in vivo, is subjected to an aqueous environment and therefore, it is important to understand the influence of this upon the mechanical integrity of experimental cements. In this current investigation the static and dynamic properties of PEMA cement, with and without 30 wt % untreated and silanated HA, were examined after periods of immersion in Ringer's solution. A commercial PMMA cement was also tested in a similar manner. Relatively small changes in static mechanical properties were observed after 12 weeks storage for the PEMA cements, the largest change being for the PEMA cement reinforced with silanated HA. The PMMA cement exhibited the largest change in static strength with a decrease of 16.6%. In contrast to these results, the fatigue properties of the PEMA cements were found to decrease significantly after storage in Ringer's solution, again with the largest changes to the PEMA cement reinforced with silanated HA. This effect was attributed to the reduction in efficiency of the silane coupling agent in the presence of water. The fatigue resistance of the PMMA cement was not reduced after immersion in a saline environment.

Journal Article↗