Search PubMed⌕ Search

SEARCH · Search PubMed

Results for “ACRYLIC RESINS”

Search indexed PubMed citations on genomics, clinical trials, systematic reviews and public health. Explore titles, authors and supplied subject terms, then open the PubMed record.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,711 records · Page 95Linked to original sources

Technical and clinical assessment of the use of a new material-based splint in orthognathic surgery.

Heat or auto-cured acrylic resins are materials that are commonly used in splint construction. Newly developed light-cured resins hold promise in view of the altered characteristics of the material. The aim of this study was to evaluate how far light-curing resin-based splints can be used in orthognathic surgery. Over a period of 1 year, 141 orthognathic surgeries were planned and performed using randomly chosen light-cured splints versus auto-polymerized splints. The performance of splint fabrication, the model planning and the clinical use were assessed by different measurements. The dental technician, the orthodontist and the surgeon evaluated objective parameters (model damage, fabrication time, accuracy of registration, adjustment time) as well as subjective criteria (handling). This study revealed that the use of light-curing splints significantly improved the accuracy (97.7% versus 81.2% in the case of acrylic materials). Less time was needed for the fabrication and adjustment of the splint. There was concomitantly less model damage to be observed when light-curing resins were used (9.2% versus 83.5%) and subjective measurements revealed significantly better handling of light-curing resin-based splints. Light-curing resin splints used in orthognathic surgery seem to be advantageous.

Acrylic Resins↗

Wear mechanisms of resin and porcelain denture teeth.

The aim of this investigation was to describe the wear mechanism in occlusal contact areas of porcelain and acrylic resin denture teeth opposing different dental materials. A 55-year-old man with earlier extensive wear was given two complete dentures, as identical as possible, in the upper jaw. One of the dentures had diatoric teeth in cross-linked resin and the other denture had diatoric teeth in porcelain. The dentures were antagonizing a new gold-acrylic fixed bridge from 46 to 36. Two contralateral segments of the bridge were made as removable double crowns. The removable segments were made in different materials: gold, porcelain, light-cured resin, and heat-cured resin. Wear of the denture teeth was studied by scanning electron microscopy on replica models made after 1 and 2 months of antagonizing contact with the various materials. Wear of both porcelain and modern cross-linked resin teeth was mainly a fatigue type of wear. Abrasion was observed when hard particles were assumed to be part of the wear debris.

Dental Porcelain↗

Protrusive positioners.

Techniques were described for fabricating maxillary and mandibular protrusive positioners for treatment of disk-condyle derangements. Treatment time with the splints varies from 4 to 12 months depending on the age of the patient, the degree of existing symptoms, and patient motivation. At the end of the treatment period and after removal of the splints, the patient may have (1) no pain or internal derangement, (2) no pain but internal derangement with or without reduction, or (3) pain and internal derangement with or without reduction. If dental treatment is required, patients in the first two categories can be treated at a physiologically acceptable treatment position with existing treatment modalities. For patients in the third category, definitive, irreversible stabilization should be reevaluated. For these patients a mandibular cast splint can be changed to an interim splint by replacing the self-polymerizing resin with Isosit (Ivoclar-Vivadent, Schaan, Liechtenstein) or heat-processed acrylic resin.

Age Factors↗

Direct resin composite veneers: masking the dark prepared enamel surface.

A technique for manufacturing direct resin composite veneers is presented. Described are the advantages of using an acrylic resin matrix, made before the preparation is begun, to copy anatomic details. An additional step to mask previously prepared dark enamel with opaquers is also described. The advantages and limitations of the procedures are discussed.

Composite Resins↗

Effectiveness of adhesive systems for a Co-Cr removable partial denture alloy.

PURPOSE: In vitro bond strengths of traditional denture base acrylic resin (Lucitone 199) to a cobalt-chromium partial denture alloy (J.D. Partial Denture Alloy) were tested using two surface pretreatments (sandblast, sandblast and electrochemical etch) with three adhesive primers: Lee Metal Primer, Acrylic Solder, and CR Inlay cement. A sandblasted group with no primer served as the control. MATERIALS AND METHODS: The alloy specimens (8.0-mm bonding diameter) were cast and invested to receive a traditional denture base resin after surface treatments (sandblasted, and sandblasted-electrochemically etched) and application of adhesive primers. The bonded specimens were stored in distilled water at 37 degrees C for 24 hours and divided into two groups. The first group was debonded in tension on a testing machine at a cross-head speed of 0.05 cm/min. The second group was subjected to thermocycling of 1,000 cycles and then tested for tensile bond strength. The force at which the bond failed was recorded, and the bond strength was calculated in megapascals (MPa). The sites of bond failure were examined, quantified under (20x) magnification, and recorded. Ten specimens were evaluated for each experimental condition for a total of 160 specimens. Data were analyzed by ANOVA with a factorial design. Means were compared by Tukey intervals at the 0.05 significance level. RESULTS: Significant differences in bond strength were observed, with primers being the most important factor, followed by pretreatment and storage and thermocycling with significant interactions. Sandblasted-electrochemically etched alloy with primers more effectively enhanced bond strength of the denture base resin to the treated alloy than sandblasted alloy with primers. Thermocycling had a greater effect on bond strength of the specimens with Acrylic Solder when compared with Lee and CR Inlay primers. The highest bond strengths (> or = 18.0 MPa) were observed for the conditions involving electrochemical etching and the priming with CR Inlay cement (both after 24 hours and thermocycling of 1,000 cycles). For primed specimens, the bond failures occurred cohesively within the primers or the denture resin and adhesively between the primers and the denture base resin, or between primers and alloy. For nonprimed, the bond failures occurred adhesively at the denture base resin-metal interface. CONCLUSIONS: Nonprimed specimens (both sandblasted and electrochemically etched) had lowest bond strength (0.4 +/- 0.1 MPa; 0.3 +/- 0.4 MPa). The bond strengths of the primed treated specimens were improved significantly. The CR Inlay-treated specimens exhibited the highest bond strength (20.6 +/- 6.3 MPa). After thermocycling for 1,000 cycles, the bond strengths of the specimens were significantly lower than the bond strengths of the specimens after 24 hours.

Acrylic Resins↗

Delayed extraoral hypersensitivity to dental composite material.

Despite their similarities to acrylic resins, composite resins have not been reported to cause allergies. This report documents the case of a patient who experienced several delayed hypersensitivity reactions associated with epoxy-based materials, including dental composite resin. Patch testing confirmed her hypersensitivity to the composite materials. Removal of the composite restorations and replacement with acrylic restorations did not trigger further allergic reactions. Dentists using composite resin materials should be aware of both the possibility of delayed extraoral manifestations of hypersensitivity to those materials and the management of these patients.

Adult↗

[A comparison of the adhesive strength of unaged and aged metal-resin bonding systems. An in vitro study].

The tensile strength and shearing strength of six bonding systems for the acrylic resin to metal bond were tested, unaltered and after cyclic thermal shock. The methods were 1) sandblasting with 50 mu and 2) 250 mu aluminium oxide granules, 3) electrolytic etching, 4) the RBS system, 5) the Sebond-MKV system, and 6) silicoating with the Kulzer Silicoater system. The materials to bond were Paladur, an autopolymerizing methacrylate, and the cobalt chromium alloy Wisil M. It was found that sandblasting gave good constant results depending on the size of the Al2O3 granules. RBS did not improve the tensile strength. The other tested systems improved the average values by a factor 3.5 in comparison to sandblasting. Silicoating showed a wide scattered range. The values of Sebond were increased and constant. After thermocycling the values were up to 30% better, but only when the recommended opaquer was not used. Sandblasting could give a good reference as baseline for comparative studies.

Acid Etching, Dental↗

The effect of glass fiber distribution on the transverse strength and surface smoothness of two denture resins.

The aim of this study was to evaluate the effect of glass fiber distribution on the transverse strength and surface smoothness of conventional heat cured acrylic and autopolymerizing acrylic of an injection-molding system. Forty rectangular (65x10x2.5 mm) acrylic test specimens were prepared from both acrylic types: 10 with 5% (w/w) 6 mm length fiber and 10 without fiber for both groups. Transverse strength test was applied to these specimens. Surface samples were taken from the broken and polished surfaces of these specimens and evaluated using SEM. The addition of fiber was found to cause a statistically significant increase in the transverse strength of the injection system's acrylic. In SEM observation it was revealed that there was good adhesion between glass fiber and both acrylic resins. The glass fibers distribution was more even in the injection system's acrylic. It is suggested that injection system's acrylic be fiber-reinforced to reduce denture fractures.

Analysis of Variance↗

Lamination of fragile documents as preliminary intervention to aqueous mass deacidification. A study on reversibility effects.

Paper lamination is a widely known method to consolidate fragile and brittle documents. Since the loss of mechanical strength of paper documents is almost completely due to their acidity, the procedure generally adopted by restorers consists of an aqueous treatment of deacidification followed by consolidation. The drawback of this method is due to the loss of paper fragments during the deacidification step, that must be therefore accurately controlled. Some preliminary experiments showed that a better and faster practice would be the lamination of paper documents with a water-resistant sheet before their immersion in the deacidification bath. The aim of this work is to evaluate the permeability, chemical stability and reversibility of the lamination sheets coated with two commercially available acrylic resins. From both gravimetric and FTIR analyses it appeared that slight modifications of the acrylic monomers led to different properties, and this behaviour can be exploited to improve the properties of lamination sheets in order to set up a reliable method of aqueous mass deacidification.

Acids↗

The effect on shear bond strength of different antimicrobial agents after acid etching.

The aim of the present study was to determine whether the application of different primers containing antibacterial agents (Micro Prime, Seal&Protect, and Gluma Desensitizer) can affect the shear bond strength (SBS) of an orthodontic resin composite. Seventy-two crowns of extracted lower human incisors were mounted in acrylic resin leaving the buccal surface of the crowns parallel to the base of the moulds. The teeth were randomly distributed into three experimental and one control group, each containing 18 teeth. In each experimental group, the primers were applied to the etched enamel surfaces. In the control group, no antibacterial primer was used. An orthodontic composite resin was applied to the surface into cylindrical-shaped plastic matrices after application of an orthodontic adhesive primer (Transbond XT). For shear bond testing, a stubby-shaped force transducer apparatus (Ultradent) was applied at a crosshead speed of 1 mm/minute to each specimen at the interface between the tooth and the composite until failure occurred. A Kruskal-Wallis one-way ANOVA and a Mann-Whitney U-test with a Bonferroni adjustment were used for statistical analysis. There was no significant difference between Seal&Protect (27.98 +/- 8.73 MPa) and the control (35.15 +/- 7.85 MPa) (P > 0.05). However, Gluma (21.61 +/- 7.96 MPa) and Micro Prime (14.89 +/- 5.55 MPa) caused a decrease in bond strength (P < 0.05). No statistically significant difference was observed between Seal&Protect and Gluma (P > 0.05). As triclosan containing Seal&Protect did not cause a significant decrease in bond strength, it can potentially be used under an orthodontic resin composite to obtain an antibacterial effect. However, further in vivo studies are required.

Acid Etching, Dental↗

The effects of cyclic stress on dental polymethylmethacrylate. II. Flexural fatigue.

Mechanisms of fatigue failure in polymers and the aims of fatigue testing have been examined, and factors affecting testing summarized. In the light of available work in several fields, parameters have been suggested for realistic flexural fatigue testing of denture base resins. A testing machine has been developed, with which the changes in properties of acrylic resin after fatigue in different environments can be studied. These changes developed gradually after 10(4) cycles and were related to the development of bulk crazing rather than to thermal effects. The amount of decay in the elastic modulus was not such that the material could have been said to have "failed".

Chemical Phenomena↗

Adhesive composite resins for artificial teeth: a laboratory investigation of bond strength to a cobalt-chromium alloy.

Adhesive resin systems are reported to improve the bond strength between resins and cast cobalt-chromium alloy. This investigation compares the behaviour of three resin systems. Cylinders and beams of cobalt-chromium, with 0.6-mm-diameter retention beads regularly cast onto the bonding surfaces, were air-abraded and ultrasonically cleaned. Resin veneers 4 mm deep on the cylinders and 2 mm on the bars were polymerized by heat and pressure or by light. Specimens were water-stored for 7 or 90 days, including thermocycling between 4, 37 and 60 degrees C, before testing in a Universal Testing Machine to examine the shear bond strength or the effect of the bonded resin spine on the flexural strength of the beams using a three-point bend test. Specimens were examined with an optical microscope to attempt to determine the nature of the failures that occurred. The investigation showed that, overall, the heat- and pressure-cured urethane dimethacrylate resin with and adhesive based upon methacrylic acid performed significantly less well than a conventional acrylic resin, or a hybrid composite resin with and adhesive monomer.

Chromium↗

Intrinsic 'soft-start' polymerisation shrinkage-kinetics in an acrylate-based resin-composite.

OBJECTIVES: A resin-composite based on multi-acrylate monomers was to be evaluated for any differences in the setting shrinkage-strain kinetics relative to more conventional formulations based on di-methacrylate monomers. METHODS: Four resin-composites were examined for shrinkage-strain over time periods up to 60 min, from initial irradiation, using a 'bonded disk' measurement device. One material was evaluated with a standard and also a two-level (low to high) blue light irradiation regime. The test material (Solitaire), and the other two controls were studied under fixed-(normal) level irradiation by blue light. Measurements were made at 23 and 37 degrees C. RESULTS: The low-high light irradiation applied to one di-methacrylate composite led to a highly significant (p < 0.001) reduction in shrinkage-strain to a minimal level for the initial 0.2 min. The fixed-level irradiation with the acrylate-composite also led to a formally identical, but intrinsic 'soft-start' shrinkage-delay regime; significant at p < 0.001. Di-methacrylate composites under the same fixed-level light regime did not exhibit shrinkage delay. Both di-methacrylate and multi-acrylate composites exhibited increases in the range 18-29% in final equilibrium shrinkage-strain by increase of specimen temperature. SIGNIFICANCE: Reductions in the rate of initial shrinkage of light-cured restoratives may have clinical benefits for restoration bond-integrity nearly as important as reductions in the final equilibrium shrinkage-strain. This may be achieved either by special light irradiation regimes (low to high, or ramped) or in favourable cases by novel monomer-composite formulations and setting chemistry (e.g. Solitaire). The bonded disk shrinkage-strain measurement technique is suitable for the elucidation of such rapid kinetic and temperature-dependent events during photo-polymerisation setting processes.

Acrylic Resins↗

[Notch effect on the fatigue strength of the denture base resin. (Part 3). Effect of reinforcement for composite material with notch (author's transl)].

The denture base which is made from the acrylic resin often occurs the fracture during function, and it is known that this fracture is mainly occured by the fatigue fracture, which is happened by the crack growth from the location of high stress. Until now, the author discussed on the fatigue properties about the specimens with semi-circular notch as the model of the remaining natural teeth, but these results are not easily applied to the design of denture base because the shape of denture base, considering its function and esthetics, is not changed. So, for the improvement of the strength of denture base, the denture base might be used the reinforcement. And, used as a trial the organic fiber as reinforcement, and their effects were investigated from the sides of the bending moment at fracture and the strain distribution occurs the fracture at the posterios palatal area, and its strength is improved 190%. And the fracture of the complete denture happens in general at the location between two central incisors, therefore this problem should be considered as the notched effect. So, reinforcing the lingual part of maxillary anterior teeth using the organic fiber, its strength is improved 53% comparing with the general complete denture. Therefore, the effects of reinforcement were enough appeared, and the improvement of the strength of denture base is very expected in dental use.

Composite Resins↗

Colorimetric monitoring of solid-phase aldehydes using 2,4-dinitrophenylhydrazine.

A simple and rapid method to achieve colorimetric monitoring of resin-bound aldehydes, based on ambient temperature reaction with 2,4-dinitrophenylhydrazine (DNPH) in the presence of dilute acid, has been developed as an adjunct to solid-phase organic synthesis and combinatorial chemistry. By this test, the presence of aldehydes is indicated by a red to dark-orange appearance, within a minute. Alternatively, resins that are free of aldehydes or in which aldehyde functions have reacted completely retain their original color. The DNPH test was demonstrated for poly(ethylene glycol)-polystyrene (PEG-PS), aminomethyl polystyrene (AMP), cross-linked ethoxylate acrylate resin (CLEAR), and acryloylated O,O'-bis(2-aminopropyl)poly(ethylene glycol) (PEGA) supports and gave results visible to the naked eye at levels as low as 18 micromol of aldehyde per gram of resin.

Acrylates↗

Functional impressions with thermoplastic materials for reline procedures.

Used as an impression material in a reline or rebase technique for a new or existing distal extension mandibular removable partial denture or mandibular complete denture, thermoplastic resin provides a denture base with uniform support under an occlusal load and a smooth nonirritating acrylic resin surface.

Dental Impression Materials↗

Reinforcement of denture base resin with glass fillers.

PURPOSE: This study evaluated the effect of short glass fibers on the transverse strength of a heat-polymerized acrylic resin denture base material. MATERIALS AND METHODS: Four groups of specimens (n = 10) were fabricated according to the ISO standard for the transverse strength test. E-glass fibers were triturated to produce short fibers of different lengths. Specimens for Group 1 (control) were made of unfilled polymethylmethacrylate (PMMA). For group 2, the PMMA powder was modified with 0.1 g of dry glass fibers. For group 3, the PMMA powder was modified with 0.1 g of silanized glass fibers. For group 4, the PMMA powder was modified with 0.2 g of silanized glass fibers. A three-point loading test was used to determine the transverse strength of the tested specimens. The fracture surface of each specimen was evaluated using SEM. RESULTS: The addition of untreated glass fibers increased the transverse strength by 11% but produced some porosity in the polymeric matrix. The addition of silane-treated glass fibers increased the transverse strength of PMMA by 28% for group 3 and by 26% for group 4, and produced a dense structure for the polymer-fiber composite. CONCLUSION: The transverse strength of PMMA can be slightly increased by the addition of short glass fibers.

Analysis of Variance↗