Search PubMed⌕ Search

SEARCH · Search PubMed

Results for “Resin Cements”

Search indexed PubMed citations on genomics, clinical trials, systematic reviews and public health. Explore titles, authors and supplied subject terms, then open the PubMed record.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 145 records · Page 8Linked to original sources

The influence of storage solution on dentin bond durability of resin cement.

OBJECTIVES: This study was conducted to determine the influence of storage solution on the bond durability of three resin cements to bovine dentin over the period of 1 year. METHODS: Ten bovine dentin specimens were tested for shear bond strength with each material (Panavia 21, Kuraray Co.; BISTITE, Tokuyama Co; MASA Bond, Sun Medical Co.) and storage mode, listed below. Four storage environments were studied as follows: water changed every day for 1 year; water unchanged for 1 year; Phosphate Buffered Saline (PBS) changed every week over 1 year; PBS unchanged for 1 year. Ten teeth were also tested for each material at 1 day as a control. The mode of failure was classified after fracture of the bonds by SEM observation. The means of the bond strengths were compared statistically by two-way ANOVA and Fisher's PLSD test (p < 0.05). Results for the mode of fracture were analyzed using the Mann-Whitney U test. RESULTS: Although there was no statistical difference in the mean bond strengths between the water and PBS storage solutions (p > 0.05) in all cements, the results for the shear bond strengths in the changed storage solution groups were significantly lower than those where the storage solution remained unchanged (p < 0.05). There were statistical differences between the 1 day results and the changed water groups among all cements (p < 0.05). SIGNIFICANCE: The storage condition influenced the long-term durability of dentin bonding with resin cements.

Adhesiveness↗

The attenuation of radiation by porcelain and its effect on polymerization of resin cements.

The influence of porcelain thickness and opacity on the polymerization of two dual activated (microfine and hybrid) and one light irradiated (hybrid) resin cements was assessed by hardness measurements. The surface microhardness values of the upper and lower surface of 1 mm thick resin cement specimens were determined. Specimens were polymerized using 40s irradiation beneath different thicknesses and opacities of porcelain discs. The results showed that increasing the thicknesses and opacity of the porcelain produced a statistically significant decrease in microhardness of the resin-based cements. The effect of attenuation is less for the microfine cement than for the hybrids. In the case of hybrid cements, the light activated material performed better than the dual activated cement.

Acrylic Resins↗

Microleakeage and resin cement film thickness of luted all-ceramic and gold electroformed porcelain-fused-to-metal crowns.

PURPOSE: The purpose of this study was to evaluate the sealing ability of single-unit all-ceramic and gold-electroformed crowns luted with a resin cement under laboratory conditions. MATERIALS AND METHODS: Thirty extracted maxillary premolars were selected. Standardized abutments were prepared for full-crown restorations with cervical margins located 1 mm below the cementoenamel junction. Samples were divided into two groups (n = 15) based on type of restorative system: Group 1: a heat-pressed all-ceramic system (IPS Empress 2, Ivoclar-Vivadent); Group 2: a gold-electroformed porcelain-fused-to-metal system (Gramm Technik). Crowns were luted with Excite DSC bonding system (Ivoclar-Vivadent) and Variolink II resin cement (Ivoclar-Vivadent) following manufacturer's instructions. After luting procedures and 700 thermal cycles (5 degrees C and 55 degrees C, 1 min dwell time), 20 specimens (n = 10 per group) were randomly selected and processed for microleakage evaluation at cervical sites. The remaining specimens (n = 5 per group) were prepared for SEM investigation on film thickness. Microleakage and film thickness data were statistically evaluated using the Mann-Whitney U-test (p < 0.05). RESULTS: Fifty percent of group 1 and 60% of group 2 samples showed leakage. For group 1, dye penetration was mostly observed between metal and resin material, while group 2 specimens showed leakage mainly between ceramic margins and resin cement. Samples from group 1 showed a cement thickness of 82 microm, while 71 microm was found for group 2. Statistically significant differences were not found between samples from the two groups. CONCLUSION: Regarding microleakage and film thickness, both restorative systems evaluated in this study performed similarly.

Bicuspid↗

Wear resistance of resin cements.

PURPOSE: To evaluate the in vitro wear resistance of four resin cements and a glass ionomer cement using a three-body wear test. MATERIALS AND METHODS: Each cement was evaluated as a direct restorative material as well as in conjunction with an inlay. All restorations were placed into cylindrical shaped cavity preparations generated on the flattened occlusal surface of human extracted molars. The bulk wear resistance of a cement was determined when tested as a direct restorative material. RESULTS: The wear resistance of all cements was greater when tested in conjunction with a resin composite inlay restoration. Although wear of a cement is dependent upon the method of testing, it was greater when combined with a less wear resistant resin composite inlay material. All of the cement materials used in this study exhibited less wear resistance than the resin composite inlays with which they were used. This in vitro wear testing system can be used as a screening test for the cement materials before a clinical study.

Analysis of Variance↗

Color stability of resin cements--an in vitro study.

The long-term success of an aesthetic restoration is predicated on numerous factors that include its color stability. As clinicians incorporate conservative tooth preparation into their restorative designs, the color stability of the underlying cement material increases in importance. This in vitro study evaluated the color stability of several commercially available resin cements under accelerated conditions. The investigation demonstrated that, under the experimental conditions, resin cements tended to change color between 1 week and 14 weeks, and their color change values increased with accelerated aging times.

Bisphenol A-Glycidyl Methacrylate↗

Temperature increase during resin cement polymerization under a ceramic restoration: effect of type of curing unit.

PURPOSE: This study measured the temperature increase induced by various types of curing units during resin cement polymerization under ceramic restorations. MATERIALS AND METHODS: The resin cement was polymerized between a ceramic specimen (diameter 5 mm, height 2 mm) and a dentin disk (diameter 5 mm, height 1 mm) with a conventional halogen light, a high-intensity halogen light, a plasma-arc light, and a light-emitting diode unit. The temperature increase was measured under the dentin disk with a J-type thermocouple wire connected to a data logger. Ten measurements were carried out for each curing unit. Difference between starting and highest temperature readings was measured, and the 10 calculated temperature changes were averaged. RESULTS: Temperature increase varied significantly depending on curing unit used. The plasma-arc light induced significantly higher temperature increases than any other curing unit. The light-emitting diode unit produced the lowest temperature changes. There were no statistically significant differences between the conventional and high-intensity halogen curing units. CONCLUSION: Polymerization with curing units characterized by high energy output (plasma-arc light) caused higher temperature changes compared to other curing units, but the temperature increase detected was not viewed as critical for pulpal health.

Analysis of Variance↗

Effect of surface treatment on the shear bond strength of three resin cements to a machinable feldspatic ceramic.

The aim of this study was to evaluate the shear bond strength of three resin cements to Vita Mark II ceramics under different pretreatments of the ceramic surface and to examine whether simplified pretreatment procedures would result in satisfying results compared to the state of the art. RelyX Unicem (RXU), Calibra (CAL), and Variolink II (VAR) were used as resin cements and bonded to machine milled feldspatic disks, pretreated in five different ways. (1) no pretreatment of the ceramic surface; (2) surface etched with hydrofluoric acid (HF); (3) ceramic surface silanized; (4) ceramic surface etched (HF) and silanized, (5) ceramic surface etched (HF), silanized, and covered with Heliobond. The shear bond strengths were measured initially, after 5000 and 10,000 thermocycles (TC). After 10,000 TC for CAL only procedure 5 resulted in a reliable adhesion median value of 10.7 MPa. VAR showed median values of 24.6, 17.2, and 18.1 MPa for pretreatments 5, 3, and 4, respectively. RXU performed 25.9, 22.0, and 11.0 MPa for procedures 5, 4, and 3, respectively. For procedure 2, RXU revealed the significantly highest value with 15.4 MPa (U-test, p = 0.05). Only RXU-luted specimens of procedure 1 survived the 10,000 thermocycles. The results revealed that a simplification of the ceramic pretreatment for VAR and RXU might be possible.

Adhesives↗

Shear bond of resin cement to post-cured hybrid composites.

Various surface treatments affected the shear bond strength of a dual-cured resin cement to a post-cured composite. Disks of post-cured composite inlay 2.0 mm thick by 10.0 mm in diameter, were mounted in acrylic cylinders. Various surface treatments were tested including: 1) smooth material; 2) treated by sandblasting (air abrasion); 3) sandblasting and etching with hydrofluoric acid (HF); 4) sandblasting and silane priming; 5) sandblasting, HF etching and silane priming; 6) HF etching alone; 7) HF etching and silane priming; and 8) silane priming alone. Specimens of dual-cured cement, 4.0 mm in diameter, were light-cured onto the prepared surfaces. The samples were stored in water at 37 degrees C for 7d before shear bond testing. The highest mean shear bond strengths were achieved for specimens with the following surface treatments: 1) by a combination of sandblasting, HF etching and silane priming; 2) sandblasting and HF etching; and 3) sandblasting and silane priming. Most bond failures in these groups were cohesive within the post-cured composite inlay disks. The bond strengths of the specimen in other groups were significantly lower and bond failures were mainly adhesive at the interface between the disk of post-cured composite and dual-cured resin cement.

Acid Etching, Dental↗

Relative gap formation of resin-cemented ceramic inlays and dentin bonding agents.

The effect of dentin bonding agents (DBAs) on contraction gap formation at the cavity floor of resin-cemented ceramic inlays was investigated. Cylindrical dentin cavities were pretreated with one of 12 DBAs before luting of ceramic inlays with a dual-curing resin cement. Measurements of cross sections revealed that mean gap widths were reduced between 21% and 80% compared with control specimens prepared without a DBA. The extent of the gap reduction depended on the type of bonding agent. None of the dentin bonding agents tested were able to completely eliminate development of interfacial gaps.

Cementation↗

The effect of various treatments on composite materials in bonding with resin cements.

The present study investigated the influence of surface treatments of composite materials using 6% hydrofluoric acid or 2% acidulated phosphate fluoride, the influence of the application of a bonding agent to the surface, and the influence of incremental curing of composite materials on the shear bonding strength between composite materials and resin cements. These results were studied statistically by analyzing variances in three-way classification and by their contributory ratios. The effects of hydrofluoric acids or acidulated phosphate fluorides on the treated surfaces of composite materials, and also the interfaces between composite materials and resin cements were further examined by mean of scanning electron microscopy (SEM). Unlike the controls, surfaces of all specimens treated with hydrofluoric acid or fluoride revealed micro-porous surfaces, but the effect of the surface treatment on the bonding strength was not equal for all the composite materials tested. The application of a bonding agent influenced some composite material, but the incremental curing of composite materials had no influence on bonding with resin cements.

Acidulated Phosphate Fluoride↗

Hardness development of dual-cured resin cements through different thicknesses of ceramics.

This study investigated the Knoop hardness of a thin layer in three dual-cured resin cements (Linkmax HV, Nexus 2, and Variolink II HV) irradiated through or not through different thicknesses (1 through 5 mm) of a machinable ceramic. Hardness was recorded at a series of time intervals up to five days, starting from the end of a light irradiation period. Increase in hardness was more rapid over the first 0.5 hour; thereafter it continued at a low rate until maximum hardness was attained. Ceramic thickness had a significant influence on hardness in all dual-cured resin cements, especially when ceramic thickness was more than 4 mm. In addition, it was noted that the polymerization of Nexus 2 seemed to be more dependent on light exposure compared with the other two materials. Variolink II HV and Linkmax HV, on the other hand, seemed to indicate the potential of being compensated by chemical curing to some degree.

Analysis of Variance↗

Effect of polymerization mode of a dual-cured resin cement on time-dependent shear bond strength to porcelain.

PURPOSE: To evaluate the shear bond strengths to porcelain and setting times of a dual-cured resin cement with light/chemical curing (dual) or chemical only curing versus time. MATERIALS AND METHODS: Variolink resin cement was bonded to specimens of etched, silanated porcelain. Groups of specimens were cured by dual cured or by chemical curing only. Shear bond strengths were recorded at 2, 3, 5, 60 minutes and 24 hours for dual cured and at 10, 20, 40, 50, 60 minutes and 24 hours for chemical-cured only after mixing. Kinetic-temperature profiles of dual and chemical curing modes of cement were calculated. RESULTS: Maximum bond strengths and time to attainment were 17.5 +/- 2.7 MPa at 60 minutes for chemical-cured and 26.1 +/- 2.3 MPa at 5 minutes for dual-cured. The peak in the kinetic-temperature setting profiles were 14.1 +/- 0.9 minutes for chemical curing and 52.2 +/- 5.2 seconds for dual curing. Dual curing provided significantly higher shear bond strengths versus chemical curing at both the 60-minute and 24-hour time periods.

Analysis of Variance↗

Effects of sodium hypochlorite and RC-prep on bond strengths of resin cement to endodontic surfaces.

There is concern that the use of sodium hypochlorite (NaOCl) and RC-Prep may lower the bond strength of resin cements. The objective of this study was to evaluate the effect of 5% NaOCl and RC-Prep treatment on the bond strength of a resin cement, C&B Metabond. Control roots (group 1) were biomechanically prepared using 0.9% NaCl as an irrigant; group 2, roots with 5% NaOCl; group 3, roots with RC-Prep; group 4, roots with 0.9% NaCl followed by 10% ascorbic acid; group 5, roots with 5% NaOCl followed by 10% ascorbic acid (pH 4); group 6, roots with 5% NaOCl followed by 10% neutral sodium ascorbate; and group 7, roots with RC-Prep followed by 10% ascorbic acid. All roots were then filled with C&B Metabond, incubated in water for 24 h, and then cross-sectioned into six 1-mm thick slabs representing cervical and middle root dentin. The slabs were trimmed and tested for tensile bond strength. The results demonstrated that both 5% NaOCl and RC-Prep produced significantly (p < 0.05) large reductions in resin-dentin bond strengths, and the reductions could be completely reversed by the application of either 10% ascorbic acid or 10% sodium ascorbate.

Analysis of Variance↗

Color stability of selected dual-cure composite resin cements.

PURPOSE: This in vitro study was conducted to determine the color stability of five dual-cure composite resin cements: Kerr Porcelite (Kerr Manufacturing Co, Romulus, NY), Jelenko PVS System (J.F. Jelenko and Co, Armonk, NY), Vivadent Heliolink (Vivadent USA, Amherst, NY), Mirage FLC (Chameleon Dental Products, Inc, Kansas City, KS), and Den-Mat Ultra Bond (Den-Mat Corp, Santa Maria, CA). MATERIALS AND METHODS: Each cement was used to lute two 10 mm circular Vita VMK porcelain disks 0.75 mm in thickness. The surfaces to be luted were sand blasted and a silane coupling agent applied. The natural glaze was unaltered. Manufacturer's directions were followed for manipulation of the cements. A jig was used during the application of the resins to control cement thickness. The samples were stored in distilled water at 37 degrees C. Using a Hunter Tristimulus Colorimeter (Hunter Associates Laboratory, Inc, Reston, VA), values were obtained for each specimen immediately, at 24 hours, and at 1, 2, 3, 4, 8, 12, 16, 20, and 24 weeks. RESULTS: An analysis of variance (ANOVA) showed significant differences for all specimens. Using the Scofield Hunter formula for identifying color differences (delta E), at 24 hours, and 24 weeks, Vivadent Heliolink showed the least color changes (24 hours delta E = 0.82, 24 weeks delta E = 0.98) and Kerr Porcelite the greatest (24 hours delta E = 3.94, 24 weeks delta E = 4.73). CONCLUSIONS: All dual-cure composite resin cements in this study showed short-term and long-term color change. Vivadent Heliolink showed the least color change, while Kerr Porcelite showed the most change.

Analysis of Variance↗

Human pulp response to resin cements used to bond inlay restorations.

OBJECTIVE: The aim of this study was to evaluate the pulp response following cementation of inlays using two different resin cements. METHODS: Deep Class V cavities were prepared on the buccal surface of 34 sound human premolars. Impressions were taken and inlays were prepared which were cemented with the following luting materials-Group 1: Rely X Unicem (3M ESPE); Group 2: Variolink II (Ivoclar Vivadent). In Group 3 (control), after lining the cavity floor with Dycal (Dentsply Caulk) the inlays were cemented with Rely X Unicem. Four additional teeth were used as an intact control group. For Variolink II, the adhesive system Excite was used as part of the cementation procedure. After 7 or 60 days, the teeth were extracted and processed for histological assessment. RESULTS: At 7 days, Rely X Unicem and Variolink II system triggered in two samples a mild and moderate inflammatory response, respectively. At 60 days, the pulpal response decreased for both groups. A discrete persistent inflammatory response occurred in Group 2 in which displacement of resin components across the dentin tubules was observed. In the control group, normal histological characteristics were observed. The inflammatory response and tissue disorganization were related to the remaining dentin thickness between the cavity floor and the pulp tissue. SIGNIFICANCE: Techniques for inlay cementation using distinct luting cements may cause specific pulpal damage. Variolink II associated with the adhesive system Excite cause more aggressive effects to the pulp-dentin complex than Rely X Unicem cement when both are used to cement inlay restorations.

Adolescent↗

Retention strength of tin plated gold inlays bonded with two resin cements.

Research has shown bonding of restorations to tooth structure to enhance retention of the restoration to increase the fracture resistance of the tooth, and to reduce microleakage. Resin cements have superior physical properties to traditional cements such as zinc phosphate. The purpose of this study was to compare the retention of gold inlays luted with two resin cements to that of those luted with zinc phosphate cement.

Acid Etching, Dental↗

The use of reinforced composite resin cement as compensation for reduced post length.

STATEMENT OF PROBLEM: Cements that yield high retentive values are believed to allow use of shorter posts. PURPOSE: This study investigated the use of reinforced composite resin cement as compensation for reduced dowel length. MATERIAL AND METHODS: The retention values of stainless steel posts (parallel-sided ParaPost and tapered Dentatus in 5-, 8-, and 10-mm lengths) luted with Flexi-Flow titanium-reinforced composite resin and zinc phosphate cements were evaluated. Single-rooted extracted human teeth with crowns (n = 120), removed at the cementoenamel junction, were randomly divided into 4 groups of 30 samples each. Different post lengths were luted with either Flexi-Flow or zinc phosphate. Each sample was placed into a specialized jig and on a tensile testing machine with a crosshead speed of 2 mm/min, applied until failure. The effect of different posts and cements on the force required to dislodge the dowels was evaluated with multiple analyses of variance (ANOVA). One-way ANOVA with Scheffé contrast was applied to determine the effect of different post lengths on the retentive failure of posts luted with the 2 agents. RESULTS: Flexi-Flow reinforced composite resin cement significantly increased retention of ParaPost and Dentatus dowels (P<.001) compared with zinc phosphate. One-way ANOVA revealed no statistically significant difference (P>.05) between mean retention of both dowels luted with Flexi-Flow for all posts length used (5 mm = 8 mm = 10 mm). Mean retention values of the groups luted with zinc phosphate showed a statistically significant difference (P<.001) for the different post lengths (10 > 8 > 5 mm). Parallel-sided ParaPost dowels demonstrated a higher mean retention than tapered Dentatus dowels (P<.001). CONCLUSION: In this study, Flexi-Flow reinforced composite resin cement compensated for the reduced length of shorter parallel-sided ParaPost and tapered Dentatus dowels.

Analysis of Variance↗

Effect of convergence angle on retention of resin-bonded retainers cemented with resinous cements.

STATEMENT OF PROBLEM: Poor retention is a common cause of failure for resin-bonded restorations. PURPOSE: This study evaluated the effect of the convergence angle of tooth preparations on retention of resin-bonded restorations, luted with adhesive and conventional resinous cements. MATERIAL AND METHODS: A total of 80 posterior retainers with four different tooth preparation angles were cemented with two different resinous cements, and retentive strength was measured. RESULTS: The results indicated that (1) increased tapering of tooth preparations resulted in loss of retention and this variable was statistically significant for both cements used when convergence angles exceeded 10 degrees and (2) sandblasted nickel-chromium retainers, combined with adhesive resins, should provide sufficient retention for posterior resin-bonded fixed partial dentures.

Adhesives↗