Search PubMed⌕ Search

SEARCH · Search PubMed

Results for “Poly T”

Search indexed PubMed citations on genomics, clinical trials, systematic reviews and public health. Explore titles, authors and supplied subject terms, then open the PubMed record.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,333 records · Page 74Linked to original sources

Concomitant adsorption of poly(ethylene oxide)-b-poly(epsilon-caprolactone) copolymers and sodium dodecyl sulfate at the silica-water interface.

Upon addition of silica to aqueous solutions of poly(ethylene oxide)-b-poly(epsilon-caprolactone) copolymers (PEO-b-PCL) and sodium dodecyl sulfate (SDS), adsorption of the solutes occurs at the silica-water interface. The amount of the adsorbed constituents has been measured by the total concentration depletion method. Small-angle neutron scattering experiments (SANS) have been carried out to investigate the structure of the adsorbed layer. Although SDS is not spontaneously adsorbed onto hydrophilic silica, adsorption is observed in the presence of PEO-b-PCL diblocks, in relation to the relative concentration of the two compounds. Conversely, SDS has a depressive effect on the adsorption of the copolymer, whose structure at the interface is modified. Copolymer desorption is however never complete at high SDS content. These observations have been rationalized by the associative behavior of PEO-b-PCL and SDS in water.

Adsorption↗

Molecular restructuring at poly(n-butyl methacrylate) and poly(methyl methacrylate) surfaces due to compression by a sapphire prism studied by infrared-visible sum frequency generation vibrational spectroscopy.

Infrared-visible sum frequency generation (SFG) vibrational spectroscopy, performed in visible wavelength total internal reflection (TIR) geometry, was used to determine the molecular structures of poly(n-butyl methacrylate) (PBMA) and poly(methyl methacrylate) (PMMA) surfaces in air and in contact with a smooth sapphire surface with and without the application of pressure. C-H vibrational resonances were probed optically to nondestructively examine the buried polymer/sapphire interfaces and obtain information about the molecular orientation in situ. These findings are contrasted with those of the same polymers cast from a toluene solution directly on the sapphire prism surface and annealed. Compared to polymer surface conformation in air, the SFG spectra of the deformed (compressed) PBMA at the sapphire interface illustrate that the ester butyl side chain restructures and tilts away from the surface normal. However, the molecular conformation in the similarly deformed PMMA at the sapphire interface is identical to that obtained in air, which is dominated by the upright-oriented ester methyl side chains. For PBMA and PMMA spin cast on sapphire and annealed, the surface structure of the undeformed PBMA at the sapphire interface is identical to that of the deformed PBMA at the sapphire interface, while the PMMA conformation is different and shows alpha-methyl group ordering. Since the glass transition temperature of PBMA is below room temperature, the rubbery state of PBMA demonstrates a melt-like behavior, evidenced by the fact that PBMA is in conformation chemical equilibrium at the sapphire surface even under compression. Due to the high glass transition temperature of PMMA, compression freezes PMMA in a metastable state, revealed by the restructured molecular conformation when annealed against the sapphire surface. The results of this study demonstrate that structural changes at buried polymer surfaces due to the application of contact pressure can be detected in situ by TIR-SFG vibrational spectroscopy.

Journal Article↗

Surfactant--polymer aggregates formed by sodium dodecyl sulfate, poly(N-vinyl-2-pyrrolidone), and poly(ethylene glycol).

The interaction of sodium dodecyl sulfate (SDS) in aqueous solution with poly(N-vinyl-2-pyrrolidone) (M(w) = 55,000 g/mol) in the presence of poly(ethylene glycol) (M(w) = 8000 g/mol) is investigated by electrical conductivity, zeta potential measurements, viscosity measurements, fluorescence spectroscopy, and small-angle X-ray scattering (SAXS). The results indicate that SDS-polymer interaction occurs at low surfactant concentration, and its critical aggregation concentration is fairly dependent on polymer composition. The polymer-supported micelles have average aggregation numbers dependent on surfactant concentration, are highly dissociated when compared with aqueous SDS micelles, and have zeta potentials that increase linearly with the fraction of PVP at constant SDS concentration. The analysis of the SAXS measurements indicated that the PVP/PEG/SDS system forms surface-charged aggregates of a cylindrical shape with an anisometry (length to cross-section dimension ratio) of about 3.0.

Journal Article↗

Influence of the foundation layer on the layer-by-layer assembly of poly-L-lysine and poly(styrenesulfonate) and its usage in the fabrication of 3D microscale features.

The layer-by-layer (LBL) assembly of a polypeptide, poly-L-lysine (PLL), with poly(styrenesulfonate) sodium salt (PSS) on flat template-stripped gold (TSG) surfaces precoated with a self-assembled monolayer of alkanethiols terminated with positive (pyridinium), negative (carboxylic acid), and neutral [hexa(ethylene glycol)] groups is investigated. Both the topography and the rate of film thickness growth are found to be strongly dependent on the initial surface foundation layer. LBL assembly of PLL and PSS on patterned TSG surfaces produced by micro contact printing leads to structurally distinct microscale features, including pillars, ridges, and wells, whose height can be controlled with nanometer precision.

Membranes, Artificial↗

Stabilization of lysozyme-incorporated polyion complex micelles by the omega-end derivatization of poly(ethylene glycol)-poly(alpha,beta-aspartic acid) block copolymers with hydrophobic groups.

To improve the stability of lysozyme-incorporated polyion complex (PIC) micelles in physiological condition, three types of hydrophobic groups, including phenyl (Phe), naphthyl (Nap), and pyrenyl (Py) terminal groups, were separately introduced to the omega-end of poly(ethylene glycol)-poly(alpha,beta-aspartic acid) block copolymers (PEG-P(Asp)). The goal was to enhance association forces between the enzyme, lysozyme, and PEG-P(Asp) carriers. Introduction of these hydrophobic groups significantly decreases micellar critical association concentration and increases the micellar tolerability against increasing NaCl concentrations. Particularly, PIC micelles formed from PEG-P(Asp) with Py groups was most stable against increasing NaCl concentrations up to 0.1 M. Significant deviation from a spherical shape for the micelles was also observed for the PEG-P(Asp)-Py system, consistent with an increased association number.

Aspartic Acid↗

Micellization of non-surface-active diblock copolymers in water. Special characteristics of poly(styrene)-block-poly(styrenesulfonate).

Strongly ionized amphiphilic diblock copolymers of poly(styrene)-b-poly(styrenesulfonate) with various hydrophilic and hydrophobic chain lengths were synthesized by living radical polymerization, and their properties and self-assembling behavior were systematically investigated by surface tension measurement, foam formation, hydrophobic dye solubilization, X-ray reflectivity, dynamic light scattering, small-angle neutron scattering, small-angle X-ray scattering, and atomic force microscope techniques. These copolymer solutions in pure water did not show a decrease of surface tension with increasing polymer concentration. The solutions also did not show foam formation, and no adsorption at the air/water interface was confirmed by reflectivity experiments. However, in 0.5 M NaCl aq solutions polymer adsorption and foam formation were observed. The critical micelle concentration (cmc) was observed by the dye solubilization experiment in both the solutions with and without added salt, and by dynamic light scattering we confirmed the existence of polymer micelles in solution, even though there was no adsorption of polymer molecules at the water surface in the solution without salt. By the small-angle scattering technique, we confirmed that the micelles have a well-defined core-shell structure and their sizes were 100-150 A depending on the hydrophobic and hydrophilic chain length ratio. The micelle size and shape were unaffected by addition of up to 0.5 M salt. The absence of polymer adsorption at the water surface with micelle formation in a bulk solution, which is now known as a universal characteristic for strongly ionized amphiphilic block copolymers, was attributed to the image charge effect at the air/water interface due to the many charges on the hydrophilic segment.

Journal Article↗

Adsorption of enantiomeric poly(lactide)s on surface-grafted poly(L-lactide).

We show that resistance of densely grafted polymer layers to adsorption of chemically identical free chains, which is known to be caused by entropic expulsion of free chains from the grafted layer, can be suppressed using the grafted and free chains of opposite stereoconfiguration. Specifically, we study adsorption of poly(L-lactide) (PLLA) and its enantiomer poly(D-lactide) (PDLA) onto layers of surface-grafted PLLA in acetonitrile and chloroform by infrared spectroscopy (IR). The grafted layers with thicknesses ranging from 7 to 35 nm are produced by ring-opening polymerization of L-lactide from hydroxyl end-groups of a self-assembled monolayer on gold. The IR data indicate that adsorption on the bare gold surface is the same for the L- and D-form of the polymer. However, covering the gold with the surface-grafted PLLA produces a significant decline in the adsorption of free PLLA and, by contrast, a strong enhancement in the adsorption of free PDLA. In addition, the IR data indicate that the adsorbed PDLA chains are stereocomplexed with the grafted PLLA chains. Thus, entropic expulsion of free chains from the grafted layer, which is responsible for the resistance of surface-grafted PLLA to adsorption of free PLLA, is suppressed in the case of free PDLA by stereocomplexation between the grafted and free chains.

Journal Article↗

Functional and surface-active membranes from poly(vinylidene fluoride)-graft-poly(acrylic acid) prepared via RAFT-mediated graft copolymerization.

Poly (vinylidene fluoride) (PVDF) with "living" poly (acrylic acid) (PAAc) side chains (PVDF-g-PAAc) was prepared by reversible addition-fragmentation chain transfer (RAFT)-mediated graft copolymerization of acrylic acid (AAc) with the ozone-pretreated PVDF. The chemical composition and structure of the copolymers were characterized by elemental analysis, Fourier transform infrared spectroscopy, and thermogravimetric analysis. The copolymer could be readily cast into pH-sensitive microfiltration (MF) membranes with enriched living PAAc graft chains on the surface (including the pore surfaces) by phase inversion in an aqueous medium. The surface composition of the membranes was determined by X-ray photoelectron spectroscopy. The morphology of the membranes was characterized by scanning electron microscopy. The pore size distribution of the membranes was found to be much more uniform than that of the corresponding membranes cast from PVDF-g-PAAc prepared by the "conventional" free-radical graft copolymerization process. Most important of all, the MF membranes with surface-tethered PAAc macro chain transfer agents, or the living membrane surfaces, could be further functionalized via surface-initiated block copolymerization with N-isopropylacrylamide (NIPAAM) to obtain the PVDF-g-PAAc-b-PNIPAAM MF membranes, which exhibited both pH- and temperature-dependent permeability to aqueous media.

Acrylic Resins↗

Counterions in poly(allylamine hydrochloride) and poly(styrene sulfonate) layer-by-layer films.

The amount of counterions in layer-by-layer (LBL) films of poly(allylamine hydrochloride) (PAH) and poly(styrene sulfonate) (PSS) has been determined with X-ray photoelectron spectroscopy (XPS) for films prepared from solutions with various NaCl concentrations. Sodium and chloride counterions are present in LBL films produced from salt solutions, which are located at the surface and in the bulk of the films. The percentage of bulk counterions increases with the ionic strength of the polyelectrolyte before reaching a constant value. The bulk sodium/sulfur percentage ratios tend to 0.8 for samples washed with pure water and for samples washed with NaCl aqueous solutions, while the bulk chlorine/nitrogen percentage ratios tend to 0.5 for the same samples. The ratio between the percentages of polyelectrolyte ionic groups lies close to unity for all samples, indicating that counterions do not contribute to charge compensation in the polyelectrolyte during the adsorption process. The presence of counterions in LBL films is explained by Manning condensation near the polyelectrolyte ionic groups, leading to inter-polyelectrolyte ionic bondings via ionic networks. It is believed that condensation leads to the formation of NaCl crystallites in these LBL films, which was confirmed by X-ray diffraction measurements.

Crystallization↗

Morphology-driven surface segregation in a blend of poly(epsilon-caprolactone) and poly(vinyl chloride).

A blend of poly(epsilon-caprolactone) (PCL) and poly(vinyl chloride) (PVC) with 90 wt % PCL was prepared. Two films of this blend, which were grown at 35 and 45 degrees C, showed the absence and presence of banded spherulites, respectively. A detailed examination conducted with time-of-flight secondary ion mass spectrometry (ToF-SIMS) found that the surface composition of the film grown at 45 degrees C was related to its structure, which was shown to contain ridges and valleys. Phase images obtained using atomic force microscopy (AFM) indicated that the ridges and valleys consisted of edge-on and flat-on lamellae, respectively. ToF-SIMS imaging revealed that PVC and PCL were located mainly on the surface of the valleys and ridges, respectively. This morphology-driven surface segregation was caused by the difference in the surface energy between the flat-on and edge-on lamellae.

Microscopy, Atomic Force↗

Disk morphology and disk-to-cylinder tunability of poly(acrylic acid)-b-poly(methyl acrylate)-b-polystyrene triblock copolymer solution-state assemblies.

Disk and cylindrical micellar assemblies were formed through self-organization of poly(acrylic acid)-b-poly(methyl acrylate)-b-polystyrene (PAA-b-PMA-b-PS) amphiphilic triblock copolymers with organic diamines as counterions in water/ tetrahydrofuran (THF) solvent mixtures. The system was investigated by means of transmission electron microscopy and cryogenic transmission electron microscopy. It was found that the assembled-state morphologies could be modified by alteration of the type and concentration of cationic diamine counterion undergoing interaction with the negatively charged, polyelectrolyte PAA corona block, the relative amount of water in the water/THF mixture, and the hydrophobic block chain length. Multivalency of the organic amine counterion was critical for disk formation. It was further demonstrated that a single block copolymer underwent disc-to-cylindrical micellar transitions reversibly with variation in the relative water/THF ratio. The ability to form disks beginning from either THF-rich or water-rich solutions indicated that the disk morphology was thermodynamically stable and that THF was important in keeping the micellar structure from becoming kinetically frozen. The nanoassemblies were produced having low size dispersities and were stable for at least one month. Intermediate structures between disks and cylinders were also observed, indicating two distinct kinetic pathways between the two micelle structures.

Journal Article↗

Poly(oxyethylene) based surface coatings for poly(dimethylsiloxane) microchannels.

Control of surface properties in microfluidic systems is an indispensable prerequisite for successful bioanalytical applications. Poly(dimethylsiloxane) (PDMS) microfluidic devices are hampered from unwanted adsorption of biomolecules and lack of methods to control electroosmotic flow (EOF). In this paper, we propose different strategies to coat PDMS surfaces with poly(oxyethylene) (POE) molecules of varying chain lengths. The native PDMS surface is pretreated by exposure to UV irradiation or to an oxygen plasma, and the covalent linkage of POE-silanes as well as physical adsorption of a triblock-copolymer (F108) are studied. Contact angle measurements and atomic force microscopy (AFM) imaging revealed homogeneous attachment of POE-silanes and F108 to the PDMS surfaces. In the case of F108, different adsorption mechanisms to hydrophilic and hydrophobic PDMS are discussed. Determination of the electroosmotic mobilities of these coatings in PDMS microchannels prove their use for electrokinetic applications in which EOF reduction is inevitable and protein adsorption has to be suppressed.

Adsorption↗

Influence of a water rinse on the structure and properties of poly(3,4-ethylene dioxythiophene):poly(styrene sulfonate) films.

Poly(3,4-ethylene dioxythiophene):poly(styrene sulfonic acid) (PEDOT:PSS) films exhibit a complex structure of interconnected conductive PEDOT domains in an insulating PSS matrix that controls their electrical properties. This structure is modified by a water rinse, which removes PSS with negligible PEDOT loss. Upon PSS removal, film thickness is reduced by 35%, conductivity is increased by 50%, and a prominent dielectric relaxation is eliminated. These results suggest that the removed PSS is not associated with PEDOT and that the conductive domain network is not substantially altered by the removal of a significant fraction of insulator. The removal of PSS may benefit organic light emitting diode fabrication by reducing acid attack on indium tin oxide electrodes and lead to more robust performance in switching circuits by extending the working frequency range.

Journal Article↗

Reversible aggregation of polystyrene-block-poly(2-vinylpyridine)-block-poly(ethylene oxide) block copolymer micelles in acidic aqueous Solutions.

Micelles of polystyrene-block-poly(2-vinylpyridine)-block-poly(ethylene oxide) (PS-PVP-PEO) were studied in acidic aqueous solutions by static and dynamic light scattering, alkalimetric titration, fluorescence correlation spectroscopy, and after deposition on a mica surface by atomic force microscopy. The PS-PVP-PEO micelles prepared by dialysis in ternary 1,4-dioxane-methanol-acidic water mixtures have a very low association number and show a strong tendency to form aggregates. The aggregation, which is promoted at low pH, seems to be fully reversible. Possible mechanisms of the aggregation are discussed. Atomic force microscopy scans of PS-PVP-PEO micelles deposited on a mica surface reveal the formation of micellar aggregates and support the general concept of aggregation upon changes in conditions and deterioration of the stability of small micelles.

Journal Article↗

Self-assembly of mixtures of block copolymers of poly(styrene-b-acrylic acid) with random copolymers of poly(styrene-co-methacrylic acid).

The effects of the addition of random copolymers of poly(styrene-co-methacrylic acid) [P(S-co-MAA)] on the self-assembly of block copolymers of poly(styrene-b-acrylic acid) (PS-b-PAA) are described. The effects of variation of five factors, including the MAA content, the weight fraction and molar mass of the P(S-co-MAA), the initial concentration of the mixture, and the length of the PAA segment in the block copolymer, were investigated. With increasing MAA content, the localization of the random copolymer in the aggregate changed from the core to the interface, which led to a morphological transition from spheres to vesicles. Vesicles, mixtures of vesicles and large spheres, and large spheres alone were formed with increasing weight fraction of the random copolymer. When the molar mass of the random copolymer was high, both rods and vesicles were observed at low water contents; otherwise, only vesicles were observed. The vesicle size increased (from 100 to 140 nm) with increasing initial polymer concentration, whereas the vesicle membrane thickness remained constant. The size of the vesicles prepared from the mixtures increased with water content but decreased with the length of PAA in the diblock.

Journal Article↗

Complexes of poly(ethylene oxide)-block-poly(L-glutamate) and diminazene.

Nanoparticles with a mean hydrodynamic radius of 16 nm and low polydispersity (P.I. = 0.1) were spontaneously formed by the complexation of poly(ethylene oxide)-block-poly(L-glutamate) (PEO-b-PLGlu) with diminazene. Only one of two possible binding sites of each diminazene molecule was involved in complexation. As determined by UV-vis difference spectra measurements, the complex binding constant is on the order of 1-2 x 10(4) M(-1). Circular dichroism measurements showed that the highly water-soluble diminazene can induce and stabilize the alpha-helical secondary structure of a PLGlu block.

Journal Article↗

Nanosized amorphous calcium carbonate stabilized by poly(ethylene oxide)-b-poly(acrylic acid) block copolymers.

Particles of amorphous calcium carbonate (ACC), formed in situ from calcium chloride by the slow release of carbon dioxide by alkaline hydrolysis of dimethyl carbonate in water, are stabilized against coalescence in the presence of very small amounts of double hydrophilic block copolymers (DHBCs) composed of poly(ethylene oxide) (PEO) and poly(acrylic acid) (PAA) blocks. Under optimized conditions, spherical particles of ACC with diameters less than 100 nm and narrow size distribution are obtained at a concentration of only 3 ppm of PEO-b-PAA as additive. Equivalent triblock or star DHBCs are compared to diblock copolymers. The results are interpreted assuming an interaction of the PAA blocks with the surface of the liquid droplets of the concentrated CaCO3 phase, formed by phase separation from the initially homogeneous reaction mixture. The adsorption layer of the block copolymer protects the liquid precursor of ACC from coalescence and/or coagulation.

Acrylic Resins↗

Aggregation behavior and thermodynamics of binding between poly(ethylene oxide)-block-poly(2-(diethylamino)ethyl methacrylate) and plasmid DNA.

The aggregation behavior and the thermodynamics of binding between poly(ethylene oxide)-block-poly(2-(diethylamino)ethyl methacrylate) (PEO-b-PDEAEMA) block copolymers and plasmid DNA were examined. Binding between the polymer and DNA were confirmed by gel electrophoresis. The high affinity between the polymer and DNA was demonstrated through the ethidium bromide (EtBr) displacement assay, and the binding was found to be related to the stoichiometric balance between the amine group of the polymer and the DNA nucleotide molar ratio (N/P molar ratio). The light scattering and TEM results showed that, at low polymer concentration, the hydrodynamic radii (R(h)) of the polymer/DNA complexes was around 90 nm; however, at sufficiently high polymer concentration, the complexes condensed to around 35 nm induced by a structural rearrangement of the amphiphilic nature of the block copolymer. The isothermal titration calorimetric results showed that the binding between the polymer and DNA is driven by a large favorable enthalpy.

Calorimetry↗