Retardation of setting of plaster of Paris by organic acids: understanding the mechanism through molecular modeling.

To develop an understanding of the action of specific formulations, the growth of gypsum crystals under the influence of retardation agents (tartaric and citric acid) has been studied using molecular modeling. Surface energies of gypsum and plaster crystal faces were calculated using established protocols. The crystal morphology predicted for gypsum crystals in the absence of retardation agents is in excellent agreement with experiment. The simulations show that only in an alkaline environment is the crystal morphology of gypsum changed by retardation agents. The simulations provide a detailed description of retardation, for example, the specific mechanisms by which tartaric and citric acid retard setting of gypsum and how they differ. At high pH meso, D(-), and L(+) tartaric acid inhibit both the growth of gypsum and the dissolution of plaster while at low pH tartaric acid and citric acid will principally inhibit the growth of gypsum. The simulations provide a molecular rationalization for a range of experimental observations and a basis for the selection of alternate retardation agents.

Journal Article↗

[Correct timing of work on a hard plaster of Paris model].

Of the individuals in Hamburg questioned, 48% waited an average of 1 to 2 hours after making a stone cast before proceeding with work on it; 38%, 1 day; and only 2%, more than 1 day. The material test however showed that 5 or 6 days of storage at room temperature are necessary before optimal values are obtained for compressive strength, ball-thrust hardness, and abrasive hardness. The greatest amount of expansion with type IV stone plaster, removed from the cast after 30 minutes, was measured between 8 and 24 hours at room temperature, after the plaster had been mixed. The least changes in dimension were recorded after a 5-day contractive phase. Given these results, the stone cast should be stored for 5 to 6 days at room temperature before work is resumed on it if precision work is to be done.

Calcium Sulfate↗