Search PubMed⌕ Search

SEARCH · Search PubMed

Results for “Haversian System”

Search indexed PubMed citations on genomics, clinical trials, systematic reviews and public health. Explore titles, authors and supplied subject terms, then open the PubMed record.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 325 records · Page 18Linked to original sources

Dependence of mechanical properties on fibre angle in narwhal tusk, a highly oriented biological composite.

The successful modelling of the mechanical properties of mineralized tissues depends critically on the knowledge of the off-axis behaviour of individual unidirectional lamellae. Information on this is lacking. In this work we attempt to rectify the situation. Young's modulus, measured in bending and tension, and the tensile strength and ultimate strain to failure of the dentine of the narwhal Monodon monoceros, were determined on specimens that had almost unidirectional fibres, whose direction differed considerably from specimen to specimen. Modulus and strength decreased steadily with the degree of off-angle loading, falling to about 45% of maximum for modulus, and 35% of maximum for strength. Ultimate strain showed a less uniform behaviour, and remained remarkably high at large angles. Differences in mechanical behaviour were not related to the very small differences in mineral content measured between specimens. These findings have strong implications for modelling the anisotropic behaviour of bone, because dentine is very much like bone in most important respects. Predictions using classical composite theory are reasonably satisfactory, as long as the mineral crystals are assumed to be platelets, not rods.

Animals↗

Osteonal structure better predicts tensile strength of healing bone than volume fraction.

Refractures and secondary fractures occur after removal of internal fixation devices even when the X-rays show well-mineralized bony unions. This indicates the unreliability of bone density as the only parameter to estimate the strength of healing bone. The aim of this study was to show that the strength of healing bone is more influenced by microstructural parameters than by bone density. A drill hole defect in the sheep tibia was used to investigate bone healing under stable conditions. After 4, 6, 9, 12, 24 and 104-week healing periods, bone specimens were taken from the healing zone and tested mechanically as well as histo-morphologically. The bone volume fraction in the defect increased at the beginning faster than the strength. In the later phase (> 24 weeks) the bone remodeling process dominated with little increase in bone volume fraction but an increase in strength. The increase in strength was linearly correlated to the orientation of the bone lamellae. Orientation of the bone lamellae which cannot be well visualized in a clinical X-ray, relates to strength more than density. Because only density and not microstructure can be well demonstrated in a clinical X-ray, a radiographically 'healed' defect may not reflect structural restoration for many years.

Animals↗

A case for bone canaliculi as the anatomical site of strain generated potentials.

We address the question of determining the anatomical site that is the source of the experimentally observed strain generated potentials (SGPs) in bone tissue. There are two candidates for the anatomical site that is the SGP source, the collagen-hydroxyapatite porosity and the larger size lacunar-canalicular porosity. In the past it has been argued, on the basis of experimental data and a reasonable model, that the site of the SGPs in bone is the collagen-hydroxyapatite porosity. The theoretically predicted pore radius necessary for the SGPs to reside in this porosity is 16 nm, which is somewhat larger than the pore radii estimated from gas adsorption data where the preponderance of the pores were estimated to be in the range 5-12.5 nm. However, this pore size is significantly larger than the 2 nm size of the small tracer, microperoxidase, which appears to be excluded from the mineralized matrix. In this work a similar model, but one in which the effects of fluid dynamic drag of the cell surface matrix in the bone canaliculi are included, is used to show that it is possible for the generation of SGPs to be associated with the larger size lacunar-canalicular porosity when the hydraulic drag and electrokinetic contribution of the bone fluid passage through the cell coat (glycocalyx) is considered. The consistency of the SGP data with this model is demonstrated. A general boundary condition is introduced to allow for current leakage at the bone surface. The results suggest that the current leakage is small for the in vitro studies in which the strain generated potentials have been measured.

Biomechanical Phenomena↗

Incidence of nutrient canals in hypertensive patients: a radiographic study.

The present study was undertaken to determine the correlation between the radiographic appearance of nutrient canals and hypertension. Comparison was made in hypertensive and nonhypertensive patients of the same age group and similar oral status. The results showed an increased incidence of nutrient canals in hypertensive patients.

Adolescent↗

The fibrous structure of bone determined by x-ray diffraction.

The fibrous structure of both primary and secondary type cortical bone is determined. The three dimensional fibrous orientation is expressed quantitatively by pole figures of the (002) diffraction. Whilst both types of bone exhibit one major axis of fibrous orientation which is aligned on average with the long axis of the femur, primary type bone exhibits a planar orientation which is consistent with a fibrous spread within the laminations but not from one lamination to the next. Secondary type bone exhibits a degree of preferred orientation with rotational symmetry about the main fibre axis.

Aged↗

Ultrasonic wave propagation and attenuation in wet bone.

The propagation of ultrasonic longitudinal waves in bovine plexiform and human Haversian bone has been studied over the range 0.5-16 MHz. In wet bone little velocity dispersion was observed, in contrast to the results of earlier studies on dry bone. Large values of attenuation were observed.

Animals↗

Bone microstructure by collagenase etching.

A novel technique has been developed for microstructural studies of bone. The spatial organizations of the mineral and collagen fibres in bone have been a matter of discussion for some time, with numerous diverse observations arising from various preparative techniques. In this latest investigation details of the mineral structure are clearly revealed in the SEM by treating a cut and polished surface of bone with collagenase to remove the major organic component. This new procedure has minimal effect on the mineral and hence reveals microstructural detail which is far closer to that in vivo than in previous investigations. This paper concentrates on two aspects of the studies, namely the detailed morphology of the mineral component and the arrangement of the collagen fibres in the osteons of compact bone. Firstly, the mineral component is revealed as comprising 'crystallites' (approximately 20 nm diam.) which aggregate to form larger contiguous 'spheroidal particles' (approximately 100 nm diam.), which in turn form 'granules' (approximately 500 nm diam.). Secondly, the regions from which collagen fibres have been removed are clearly revealed, showing that within an osteon, alternating lamellae have collagen fibres oriented approximately parallel to and circumferential to the Haversian canal respectively.

Animals↗

The relative accuracy and reliability of histological aging methods.

Histological aging methods of Kerley and of Ahlqvist and Damsten were applied to bone samples from thirteen individuals of known age at death. Relative accuracy and reliability were determined for six of Kerley's predicting formulas for the femur, fibula and tibia, and his profile method, Ahlqvist and Damsten's femoral predicting formulas, and age determined by averaging ages predicted by Kerley's six formulas. Averaging age estimates by Kerley's six formulas (mean regression) was found to produce the overall greatest accuracy and reliability. Dividing the sample into two age groups (13 - 51 and 60 - 102 years) altered the results only slightly. Kerley's femoral intact osteon formula produced the greatest accuracy for individuals in the younger age category, while his fibular osteon fragment formula was most accurate for older ages. Mean regression produced the greatest reliability for all age classes. Based upon both accuracy and reliability, averaging age predictions by Kerley's regression formulas appears to be the method of choice for broad application of histological aging.

Adolescent↗

Study on the microstructures of skull fracture.

The authors observed the edges of skull fractures under the scanning electron microscope. Many microfractures can be found along the main fracture lines. The width of the microfractures varies from 5 to 100 microns. They may be located either in the external compact bone or between the outer compact bone and diplöe, or in the diplöe. Those within the diplöe form transverse, longitudinal or spiral fractures of bony trabeculae. Collagenous fibre bunches in the bony matrix may be divided or broken and the different layers of collagenous fibre may be separated. The blood vessels inside the skull may be crosscut or longitudinally torn by the fracture lines. Sometimes the torn blood vessels may be drawn out of the Haversian canals. In antemortem fractures, the fibrin networks and red blood cells can be easily found in the depths of those cracks. The possible mechanism of formation of the microfractures and the possibility of differentiation between ante- and post-mortem fractures are discussed.

Animals↗

On the significance of remodeling space and activation rate changes in bone remodeling.

This paper quantifies the relative contributions of the remodeling space and the accumulation of Haversian canals to bone porosity at various ages. It also examines the importance of variations in the rate of bone remodeling that occur during growth and aging, and as a result of trauma and disease. The dependence of the remodeling space (cavities due to resorbing, reversing, and refilling BMUs) and the Haversian canal components of porosity on the Basic Multicellular Unit (BMU) activation frequency are mathematically formulated. A graph is developed using data for the cortex of the human rib which shows the extent to which porosity is primarily due to the remodeling space in children, and to accumulated Haversian canals in adults. It is shown that the diminution of activation frequency between birth and age 35 contributes to the concurrent increase in bone volume fraction, and the increase in activation frequency after age 35 contributes to the subsequent decline of bone volume fraction. An equation is derived for determining the time rate of change of activation frequency using two fluorochrome labels.

Aging↗

Evidence of strain-mode-related cortical adaptation in the diaphysis of the horse radius.

The relative importance that certain strain features, including mode (e.g., tension vs. compression) and magnitude, have in affecting adaptive bone remodeling seen in normal skeletally mature bones remains controversial. The equine radius is used as a model because in vivo strain data show that the mid-to-proximal diaphysis receives a consistent history of predominantly cranial-caudal bending loads, in contrast to the distal diaphysis which receives relatively more torsional loading superimposed on cranial-caudal bending. Medial and lateral cortices serve as control regions because they correspond to a neutral axis of bending. Equine radii were sectioned transversely at 65% (proximal), 50%, and 35% (distal) of length and cortical bone from the cranial ("tension"), caudal ("compression"), medial, and lateral regions was examined to determine if one, of many, structural and material features could be distinguished as being consistently related to the distribution of the prevailing strain modes. Mineral content (percent ash) differences, though statistically significant (p < 0.01), vary less than 1% between regions of the cortex at all sections. Porosity is not significantly different between any of the regions (p = 0.13). In the 65% and 50% sections, secondary osteon population density (OPD, osteons per square millimeter) and fractional area of secondary bone (FASB) are each nearly two times as great in the caudal regions than in the other three regions (p < 0.01). The 35% section shows a pattern opposite of that in the other sections--there are more than two times as many osteons in the cranial cortex than in the caudal cortex.(ABSTRACT TRUNCATED AT 250 WORDS)

Animals↗

Osteonal structure in the equine third metacarpus.

In studying the flexural fatigue properties of the equine third metacarpal (cannon) bone, we previously found that the dorsal region was weaker monotonically, but more fatigue resistant, than the lateral region. Fatigue resistance was associated with fracture surfaces which demonstrated that secondary osteons had "pulled out" of the surrounding matrix; this never happened in lateral specimens. We therefore became interested in the osteonal structure of this bone, and began to study its birefringence patterns in circularly polarized light. We found that the predominant type of secondary osteon was one in which only the outermost few lamellae were circumferential, with the inner lamellae being longitudinally oriented. This "hoop" pattern had not been described in Ascenzi's classic papers. Using basic fuchsin-stained, undecalcified cross-sections from the dorsal, medial, and lateral midshaft regions of 12 pairs of cannon bones, we classified 360 secondary osteons according to their birefringence patterns, and measured their inner and outer diameters. We found that variants of the hoop category comprised 60% of all osteons, but were significantly less common in the dorsal region, where the predominant types were Ascenzi's "longitudinal" or "alternating" patterns. The dorsal region also had smaller osteons (OD = 156 +/- 19 microns) than the medial (179 +/- 13 microns, p = 0.0004) and lateral (182 +/- 13 microns, p = 0.0001) regions. We postulate that these regional variations in osteonal size and structure, which are obviously produced by regional variations in remodeling, have important mechanical implications.

Analysis of Variance↗