Preparation of poly(DL-lactide-co-glycolide) nanoparticles by modified spontaneous emulsification solvent diffusion method.

PURPOSE: The objectives of this study were to establish a new preparation method for poly(DL-lactide-co-glycolide) (PLGA) nanoparticles by modifying the spontaneous emulsification solvent diffusion (SESD) method and to elucidate the mechanism of nanoparticle formation on the basis of the phase separation principle of PLGA and poly(vinyl alcohol) (PVA) in the preparation system. METHODS: PLGA nanoparticles were prepared by the modified-SESD method using various solvent systems consisting of two water-miscible organic solvents, in which one solvent has more affinity to PLGA than to PVA and the other has more affinity to PVA than to PLGA. The yield, particle size, size distribution and PVA content of the PLGA nanoparticles were evaluated, and the phase separation behaviors of the polymers were elucidated. RESULTS: The modified-SESD method provided a good yield of PLGA nanoparticles over a wide range of composition ratios in the binary mixture of organic solvents. Several process parameters, including the fed amount of PLGA, PLGA concentration and PVA concentration were examined to achieve the optimum preparation conditions. The discrete powder of PLGA nanoparticles was obtained by freeze-drying. No change in the PVA content of PLGA nanoparticles was observed even after several times of washing treatment by ultrafiltration, suggesting a strong surface adsorption. It was found that the appropriate selections of binary solvent mixtures and polymeric concentrations in both organic and aqueous phases could provide excellent yield and favorable physical properties of PLGA nanoparticles. CONCLUSION: The proposed modified-SESD method can be used to provide PLGA nanoparticles of satisfactory quality at an acceptable yield for industrial purposes.

Diffusion↗

Folate-conjugated iron oxide nanoparticles for solid tumor targeting as potential specific magnetic hyperthermia mediators: synthesis, physicochemical characterization, and in vitro experiments.

New folate-conjugated superparamagnetic maghemite nanoparticles have been synthesized for the intracellular hyperthermia treatment of solid tumors. These ultradispersed nanosystems have been characterized for their physicochemical properties and tumor cell targeting ability, facilitated by surface modification with folic acid. Preliminary experiments of nanoparticles heating under the influence of an alternating magnetic field at 108 kHz have been also performed. The nanoparticle size, surface charge, and colloidal stability have been assessed in various conditions of ionic strength and pH. The ability of these folate "decorated" maghemite nanoparticles to recognize the folate receptor has been investigated both by surface plasmon resonance and in folate receptor expressing cell lines, using radiolabeled folic acid in competitive binding experiments. The specificity of nanoparticle cellular uptake has been further investigated by transmission electron microscopy after incubation of these nanoparticles in the presence of three cell lines with differing folate receptor expression levels. Qualitative and quantitative determinations of both folate nanoparticles and nontargeted control nanoparticles demonstrated a specific cell internalization of the folate superparamagnetic nanoparticles.

Cell Line, Tumor↗

Ligand density effect on biorecognition by PEGylated gold nanoparticles: regulated interaction of RCA120 lectin with lactose installed to the distal end of tethered PEG strands on gold surface.

PEGylated gold nanoparticles (diameter: 20 nm) possessing various functionalities of lactose ligand on the distal end of tethered PEG ranging from 0 to 65% were prepared to explore the effect of ligand density of the nanoparticles on their lectin binding property. UV-visible spectra of the aqueous solution of the nanoparticles revealed that the strong steric stabilization property of the PEG layer lends the nanoparticles high dispersion stability even under the physiological salt concentration (ionic strength, I = 0.15 M). The number of PEG strands on a single particle was determined to be 520 from thermogravimetric analysis (TGA). Scanning electron microscopy (SEM) observation under controlled acceleration voltage revealed the thickness of the PEG layer on the nanoparticle to be approximately 7 nm. The area occupied by a single lactose molecule on the surface of PEGylated gold nanoparticles was then calculated based on TGA and SEM results and was varied in the range of 10-34 nm2 depending on the lactose functionality (65 approximately 20%). PEGylated gold nanoparticles with 40% and 65% lactose functionality showed a selective and time-dependent aggregation in phosphate buffer with the addition of Ricinus communis agglutinin (RCA120) lectin, a bivalent galactose-specific protein. The aggregates can be completely redispersed by adding an excess amount of galactose. Time-lapse monitoring of UV-visible spectra at 600-750 nm revealed that the aggregation of PEGylated gold nanoparticles was accelerated with an increase in both RCA120 concentration in the solution and the lactose density of the nanoparticles. Furthermore, the sensitivity of lectin detection could be controlled by the regulation of lactose density on the particle surface. Interestingly, there was a critical lactose density (>20%) observed to induce detectable particle aggregation, indicating that the interaction between the particles is triggered by the multimolecular bridging via lectin molecules.

Dimerization↗

Ethylene glycol monolayer protected nanoparticles for eliminating nonspecific binding with biological molecules.

The usefulness of the hybrid materials of nanoparticles and biological molecules in many occasions depends on how well one can achieve a rational design based on specific binding and programmable assembly. Nonspecific binding between nanoparticles and biomolecules is one of the major barriers for achieving its utilities in a biological system. In this paper, we demonstrate a new approach to eliminate nonspecific interactions between nanoparticles and proteins by synthesizing ethylene glycol protected gold nanoparticles. We discovered that with the water content optimized in the range of 9-18% in the reaction mixture, di-, tri-, and tetra(ethylene glycol) protected gold nanoparticles Au-S-EGn (n = 2, 3, and 4) could be directly synthesized. These gold nanoparticles that are bonded with a uniform monolayer with defined length varying from 0.8 to 1.6 nm (from molecular modeling) have great stability in aqueous solutions with a high concentration of electrolyte and organic solutions. Using ion-exchange chromatography and gel electrophoresis, we demonstrated that these Au-S-EGn (n = 2, 3, or 4) nanoparticles have complete resistance to protein nonspecific interactions. These types of nanoparticles provide a fundamental starting material for designing hybrid materials composed of metallic nanoparticles and biomolecules.

Biocompatible Materials↗

A modular nanoparticle-based system for reagentless small molecule biosensing.

Metalloprotein tethered CdSe nanoparticles have been generated to provide selective and reagentless maltose biosensing. As opposed to cell or protein detection by semiconducting nanoparticle bioconjugates, a modular method for small-molecule detection using semiconducting nanoparticle bioconjugates has been difficult. Here we report a method for reagentless protein-based semiconducting nanoparticle biosensors. This method uses Ru(II) complex-CdSe nanoparticle interactions and the maltose-induced conformation changes of maltose binding protein to alter the CdSe nanoparticle fluorescence emission intensity. In this proof-of-principle system, the maltose-induced protein conformation changes alter the Ru(II) complex-CdSe nanoparticle interaction, which increases the CdSe emission intensity. Altered CdSe emission intensity effects are best described as electron transfer from the Ru(II) complex to the CdSe excited state forming the nonfluorescent CdSe anion. Four surface-cysteine, Ru(II) complex-attached maltose-binding proteins have been studied for maltose dependent alteration of CdSe emission intensities. With 3.0-3.5 nm diameter CdSe nanoparticles, all ruthenated maltose-binding proteins display similar maltose-dependent increases (1.4-fold) in CdSe emission intensity and maltose binding affinities (KA = 3 x 106 M-1). For these four systems, the only difference was the sample-to-sample variation in maltose-dependent responses. Thus, very few surface cysteine mutations need to be examined to find a successful biosensor, as opposed to analogous systems using organic fluorophores. This strategy generates a unimolecular, or reagentless, semiconducting nanoparticle biosensor for maltose, which could be applied to other proteins with ligand-dependent conformation changes.

Biosensing Techniques↗

Raman studies on the interaction of the reactants with the platinum nanoparticle surface during the nanocatalyzed electron transfer reaction.

Raman studies are conducted to understand the specific interactions between the individual reactants and the platinum nanoparticle surface during the nanocatalyzed electron transfer reaction between hexacyanoferrate (III) ions and thiosulfate ions. When Pt nanoparticles are added to the thiosulfate ion solution, a shift in the symmetric SS stretching mode is observed compared to the frequency observed for the free thiosulfate ions in solution, suggesting that binding to the Pt nanoparticle surface occurs via the S- ion. It is also observed that there are no shifts in the symmetric and asymmetric OSO bending or SO stretching frequencies. This suggests that the thiosulfate ions do not bind to the nanoparticle surface via the O- ion. When platinum nanoparticles are added to the hexacyanoferrate(III) ion solution, evidence is found for both adsorbed hexacyanoferrate(III) ions and a platinum cyanide complex. For adsorbed hexacyanoferrate(III) ions, the CN stretching frequency is observed at 2101 cm(-1) and the Fe-C stretching frequency is found at 368 cm(-1). The observed CN stretching frequencies located at 2147 and 2167 cm(-1) provide strong evidence that there is a Pt(CN)4(2-) platinum cyanide complex formed. In addition, the Pt-CN band is also observed at 2054 cm(-1). These observed bands provide spectroscopic evidence that the hexacyanoferrate(III) ions dissolve by forming a complex with the surface platinum atoms of the nanoparticles. Raman spectra of the product mixtures are obtained after the completion of the reaction when carried out with higher reactant concentrations to observe the Raman spectra, but with a similar 10:1 ratio of thiosulfate to hexacyanoferrate(III) ions as used previously, with and without PVP-Pt nanoparticles at a correspondingly higher concentration. It is observed that there are no shifts in the characteristic Raman bands associated with hexacyanoferrate(II) ions and no evidence for the formation of adsorbed hexacyanoferrate(II) species or platinum cyanide complexes in the presence of the platinum nanoparticles. In addition, there is evidence for the shifted symmetric SS stretching mode, suggesting that some of the unreacted thiosulfate (present in large excess) is bound to the Pt nanoparticle surface. Thus, under the actual reaction conditions, the hexacyanoferrate(III) ions preferentially react with adsorbed thiosulfate ions to form the reaction products, and this supports the surface catalytic mechanism we proposed previously.

Journal Article↗

Size-dependent ultrafast electronic energy relaxation and enhanced fluorescence of copper nanoparticles.

The energy relaxation of the electrons in the conduction band of 12 and 30 nm diameter copper nanoparticles in colloidal solution was investigated using femtosecond time-resolved transient spectroscopy. Experimental results show that the hot electron energy relaxation is faster in 12 nm copper nanoparticles (0.37 ps) than that in 30 nm copper nanoparticles (0.51 ps), which is explained by the size-dependent electron-surface phonon coupling. Additional mechanisms involving trapping or energy transfer processes to the denser surface states (imperfection) in the smaller nanoparticles are needed to explain the relaxation rate in the 12 nm nanoparticles. The observed fluorescence quantum yield from these nanoparticles is found to be enhanced by roughly 5 orders of magnitude for the 30 nm nanoparticles and 4 orders of magnitude for the 12 nm nanoparticles (relative to bulk copper metal). The increase in the fluorescence quantum yield is attributed to the electromagnetic enhancement of the radiative recombination of the electrons in the s-p conduction band below the Fermi level with the holes in the d bands due to the strong surface plasmon oscillation in these nanoparticles.

Journal Article↗

Bimetallic (Ag)Au nanoparticles prepared by the seed growth method: two-dimensional assembling, characterization by energy dispersive X-ray analysis, X-ray photoelectron spectroscopy, and surface enhanced raman spectroscopy, and proposed mechanism of growth.

Layered core-shell bimetallic silver-gold nanoparticles were prepared by overdeposition of Au over Ag seeds by the seed-growth method using tetrachloroauric acid, with hydroxylamine hydrochloride as the reductant. The effects of pH, reduction rate, and seeding conditions on the morphology and surface plasmon extinction of the bimetallic nanoparticles were investigated. Nanoparticles prepared by a rapid reduction in the neutral ambient and assembled into two-dimensional nanoparticulate films by adsorption of 2,2'-bipyridine were characterized by energy-dispersive X-ray analysis, X-ray photoelectron spectroscopy, surface-enhanced Raman scattering spectroscopy, and transmission electron microscopy. The results are consistent with Ag core and Ag/Au-alloyed shell composition of the nanoparticles. Evidence of the presence of Ag on the surface of the nanoparticles, of enrichment of the Ag/Au alloy shell by Ag toward or at the nanoparticle surface, and of modification of the nanoparticle surface by adsorbed chlorides is also provided. Reduction of the size of the Ag seeds, alloying of Ag and Au in the shell of the nanoparticles, and modification of their surfaces by adsorbed chlorides are tentatively attributed to positive charging of the nanoparticles during the electrocatalytic overdeposition of Au over Ag seeds.

Journal Article↗

Alkanethiol-induced structural rearrangements in silica-gold core-shell-type nanoparticle clusters: an opportunity for chemical sensor engineering.

Electrostatically bonded SiO2.Au nanoparticle clusters form by reaction of 3-aminopropylsilane-modified SiO2 spheres (470 nm) with citrate-coated gold nanoparticles (9.7 nm) in water. Reaction of the clusters with 0.01 M KBr or HCl solution induces desorption of the gold nanoparticles within minutes. Reaction of the clusters with alkanethiols CnH2n+1SH (n = 2-18) at 80 degrees C causes the gold nanoparticles to form stringlike gold nanoparticle structures for thiols with short alkane groups (n = 2, 3, 4) and hexagonally packed arrays of gold nanoparticles for thiols with long alkane groups (n = 5-18) on the silica surfaces. The structural changes indicate that the bonding between Au and SiO2 nanoparticles has changed from electrostatic to van der Waals. Elemental analyses show that the reaction with hexanethiol does not affect the Au/Si/O composition of the SiO2.Au cluster, and Raman spectra on the hexanethiol-reacted cluster indicate the formation of a thiol SAM on the gold nanoparticles. The thiol-reacted SiO2.Au clusters display characteristic shifts of the absorption maxima in the visible spectra, and there is an inverse relation between these shifts and the lengths of the alkyl groups in the thiols. This relationship can be understood in terms of the free electron model for metals. The use of SiO2.Au nanoparticle clusters as coulometric sensors for the qualitative detection of thiols is discussed.

Journal Article↗

Synthesis of high surface area hydroxyapatite nanoparticles by mixed surfactant-mediated approach.

A new surfactant-mediated approach was developed to synthesize hydroxyapatite (HAp) nanoparticles with high surface areas by calcination of their precursors encapsulated with calcium stearate using mixed surfactant-containing reaction mixtures. Acidic aqueous solution of calcium phosphate was mixed with both or either nonaoxyethylene dodecyl ether (C12EO9) and polyoxyethylene(20) sorbitan monostearate (Tween 60) and then was treated with aqueous ammonium at 25 degrees C. The C12EO9-based single surfactant system yielded an aggregate of platy HAp nanoparticles 20-40 nm in size, whereas the Tween 60-based single and mixed systems led to lath-shaped HAp nanoparticles 2-8 nm wide and encapsulated with calcium stearate. On calcination at 500 degrees C, the stearate-encapsulated HAp nanoparticles in the latter two systems were deorganized into high surface area HAp nanoparticles. Particularly, the HAp nanoparticles in the mixed system exhibited a specific surface area as high as 364 m2 g(-1) that is roughly 3 times larger than 160 m2 g(-1) for those in the single system. The significantly high surface area for the former is attributed to much less adhesion of decapsulated HAp nanoparticles, which originated from the particle-separating effect of the C12EO9 molecules adsorbed on the outer surface of the stearate-encapsulated HAp nanoparticles to inhibit their agglomeration or interfacial coordination. The present results demonstrate that the mixed use of two different surfactants as a source of encapsulating and templating agent and a particle-separating agent is specifically effective for the synthesis of high surface area HAp nanoparticles.

Journal Article↗

Assessment of 4-(dimethylamino)pyridine as a capping agent for gold nanoparticles.

Gold nanoparticles stabilized with 4-(dimethylamino)pyridine (DMAP) were prepared by ligand exchange and phase transfer (toluene/water) of functionalized gold nanoparticles. DMAP-protected gold nanoparticles are water-soluble, positively charged, and fairly monodisperse (6.2 +/- 0.9 nm). To understand the scope of this interesting system, the details of the binding of DMAP to gold nanoparticles were investigated. The adsorption of DMAP onto gold surfaces was studied by electrochemistry and surface plasmon resonance. It is concluded that of the three most likely binding modes, the one involving the pyridine nitrogen binding to the gold surface, as suggested previously (Gittins, D. I.; Caruso, F. Angew. Chem., Int. Ed. 2001, 40, 3001), is consistent with experimental data. Other 4-substituted pyridines were also assessed as capping agents. The solubility in toluene and basicity of the incoming ligand, as well as the ability to form charged nanoparticles, determine whether ligand exchange and subsequent phase transfer of the nanoparticles occur. The solubility and stability of the DMAP-protected gold nanoparticles were studied as a function of pH using UV-visible spectroscopy and transmission electron microscopy (TEM). These nanoparticles are soluble and stable over a wide pH range (5.0-12.8). It was found that excess DMAP is necessary for both the preparation and the stability of the DMAP-protected gold nanoparticles.

Journal Article↗

Phase behavior and 3D structure of strongly attractive microsphere-nanoparticle mixtures.

We investigate the phase behavior and 3D structure of strongly attractive mixtures of silica microspheres and polystyrene nanoparticles. These binary mixtures are electrostatically tuned to promote a repulsion between like-charged (microsphere-microsphere and nanoparticle-nanoparticle) species and a strong attraction between oppositely charged (microsphere-nanoparticle) species. Using confocal fluorescence scanning microscopy, we directly observe the 3D structure of colloidal phases assembled from these mixtures as a function of varying composition. In the absence of nanoparticle additions, the charged-stabilized microspheres assemble into a polycrystalline array upon sedimentation. With increasing nanoparticle volume fraction, nanoparticle bridges form between microspheres, inducing their flocculation. At even higher nanoparticle volume fractions, the microspheres become well coated with nanoparticles, leading to their charge reversal and subsequent restabilization. We demonstrate how this fluid-gel-fluid transition can be utilized to control the morphology of the colloidal phases formed under gravity-driven sedimentation.

Journal Article↗

Adsorption characteristics of thionine on gold nanoparticles.

Adsorption characteristics of thionine on gold nanoparticles have been studied by using UV-vis absorption spectroscopy, fluorescence spectroscopy, transmission electron microscopy (TEM), cyclic voltammetry and Fourier transform infrared spectroscopy. With the increasing concentration of gold nanoparticles, the absorption peak intensity of H-type dimers of thionine increases continuously, whereas that of monomers of thionine first increases and then decreases. The addition of gold nanoparticles makes the equilibrium between the monomer and H-type dimer forms of thionine move toward the dimer forms. Furthermore, the adsorption behavior of thionine on gold nanoparticles is also influenced by temperature. TEM images show that the addition of thionine results in an obvious aggregation, and further support the absorption spectral results. The fluorescence intensity of adsorbed thionine is quenched by gold nanoparticles due to the electronic interaction between thionine molecules and gold nanoparticles. Cyclic voltammetric and infrared spectroscopic studies show that the nitrogen atoms of both of the NH2 moieties of thionine strongly bind to the gold nanoparticle surfaces through the electrostatic interaction of thionine with gold nanoparticles. For 15-20 nm particles, the number of adsorbed thionine molecules per gold nanoparticle is about 7.66 x 10(4). Thionine molecules can not only bind to a particle to form a compact monolayer via both of the NH2 moieties, but they can also bind to two particles via their two NH(2) moieties, respectively.

Journal Article↗

Molecular dynamics simulation of nanoparticle self-assembly at a liquid-liquid interface.

We have used molecular dynamics simulations to investigate the in situ self-assembly of modified hydrocarbon nanoparticles (mean diameter of 1.2 nm) at a water-trichloroethylene (TCE) interface. The nanoparticles were first distributed randomly in the water phase. The MD simulation shows the in situ formation of nanoparticle clusters and the migration of both single particles and clusters from the water phase to the trichloroethylene phase, possibly due to the hydrophobic nature of the nanoparticles. Eventually, the single nanoparticles or clusters equilibrate at the water-TCE interface, and the surrounding liquid molecules pack randomly when in contact with the nanoparticle surfaces. In addition, the simulations show that the water-TCE interfacial thickness analyzed from density profiles is influenced by the presence of nanoparticles either near or in contact with the interface but is independent of the number of nanoparticles present. The nanoparticles, water molecules, and TCE molecules all exhibit diffusion anisotropy.

Journal Article↗

Comparative studies on electrogenerated chemiluminescence of luminol on gold nanoparticle modified electrodes.

Comparative studies on the electrogenerated chemiluminescence (ECL) behavior of luminol on various electrodes modified with gold nanoparticles of different size were carried out in neutral solution by conventional cyclic voltammetry (CV). The results demonstrated that the gold nanoparticle modified electrodes could generate strong luminol ECL in neutral pH conditions. The catalytic performance of gold nanoparticle modified electrodes on luminol ECL depended not only on the gold nanoparticles but also on the substrate. Gold electrode and glassy carbon electrode were the most suitable substrates for the self-assembly of gold nanoparticles. Moreover, the gold nanoparticle modified gold and glassy carbon electrode had satisfying stability and reproducibility and did not need tedious pretreatment of electrode surface before each measurement. It was also found that luminol ECL behavior depended on the size of gold nanoparticles. The most intense ECL signals were obtained on a 16-nm-diameter gold nanoparticle modified electrode. The modified electrode prepared by the self-assembly method exhibited much better catalytic effect on luminol ECL than that prepared by the electrically deposited method. The ECL behavior of luminol on a gold nanoparticle self-assembled gold electrode was also investigated by other transient-state electrochemical techniques, such as chronoamperometry, differential pulse voltammetry, normal pulse voltammetry, and square wave voltammetry. The strongest ECL intensity was obtained under square wave voltammetric condition.

Journal Article↗

Long-circulating PEGylated polycyanoacrylate nanoparticles as new drug carrier for brain delivery.

PURPOSE: The aim of this study was to evaluate the ability of long-circulating PEGylated cyanoacrylate nanoparticles to diffuse into the brain tissue. METHODS: Biodistribution profiles and brain concentrations of [14C]-radiolabeled PEG-PHDCA, polysorbate 80 or poloxamine 908-coated PHDCA nanoparticles, and uncoated PHDCA nanoparticles were determined by radioactivity counting after intravenous administration in mice and rats. In addition, the integrity of the blood-brain barrier (BBB) after nanoparticles administration was evaluated by in vivo quantification of the diffusion of [14C]-sucrose into the brain. The location of fluorescent nanoparticles in the brain was also investigated by epi-fluorescent microscopy. RESULTS: Based on their long-circulating characteristics, PEGylated PHDCA nanoparticles penetrated into the brain to a larger extent than all the other tested formulations. Particles were localized in the ependymal cells of the choroid plexuses, in the epithelial cells of pia mater and ventricles, and to a lower extent in the capillary endothelial cells of BBB. These phenomena occurred without any modification of BBB permeability whereas polysorbate 80-coated nanoparticles owed, in part, their efficacy to BBB permeabilization induced by the surfactant. Poloxamine 908-coated nanoparticles failed to increase brain concentration probably because of their inability to interact with cells. CONCLUSIONS: This study proposes PEGylated poly (cyanoacrylate) nanoparticles as a new brain delivery system and highlights two requirements to design adequate delivery systems for such a purpose: a) long-circulating properties of the carrier, and b) appropriate surface characteristics to allow interactions with BBB endothelial cells.

Acrylic Resins↗

Near infrared with principal component analysis as a novel analytical approach for nanoparticle technology.

PURPOSE: To progress in the characterization of a poly(MePEGcyanoacrylate-co-hexadecylcyanoacrylate) (poly(PEGCA-co-HDCA) copolymer and the nanoparticles formed from this copolymer. METHODS: Poly(PEGCA-co-HDCA) at a MePEG/hexadecyl ratio of 1:4 was investigated by 1H-NMR and near infrared spectroscopy. The nanoparticle suspensions, obtained by the methods of nanoprecipitation or emulsion--solvent evaporation, as well as the crude nanoparticles and their dispersion medium--were analyzed by MePEG measurement, 1H-NMR, and near infrared spectroscopy. RESULTS: The 1H-NMR results showed that the (poly(PEGCA-co-HDCA) copolymer obtained bore lateral hydrophilic MePEG chains and lateral hydrophobic hexadecyl chains in a final ratio of 1:4. However, this ratio, although reproducible from batch to batch, represented only a mean value for different molecular species. Indeed, our results demonstrated the formation of more hydrophobic poly(alkyl-cyanoacrylate) oligomers (with a higher content of hexadecyl chains) and other more hydrophilic oligomers (with a higher MePEG content). Only the more hydrophobic oligomers were able to form solid pegylated nanoparticles. As far as these nanoparticles were concerned, determination of their MePEG content allowed the calculation of a distance of 1.2 nm and 1.05 nm between 2 grafted MePEG chains at the nanoparticle surface, when obtained by nanoprecipitation and emulsion-solvent evaporation, respectively. Moreover, when the same copolymer batch was used, different nanoparticles were obtained according to the preparation method, as seen by near infrared spectroscopy. CONCLUSIONS: The nanoparticles obtained by nanoprecipitation or emulsion-solvent evaporation of poly(PEGCA-co-HDCA) 1:4 copolymer displayed a different supramolecular organization, as evidenced by the near infrared spectroscopy results. Moreover, these nanoparticles showed surface characteristics compatible with a long circulating carrier.

Colloids↗

Polymeric drug nanoparticles prepared by an aerosol flow reactor method.

PURPOSE: Our purpose was to study the possibility of using a novel method, namely, aerosol flow reactor method, for the preparation of drug-containing nanoparticles with varying amounts of drug and polymer. The physical properties of the prepared nanoparticles were analyzed. METHODS: The nanoparticle size distributions were measured using differential mobility analyzer. The structure of the prepared nanoparticles was assessed by x-ray diffraction, differential scanning calorimetry, and electron microscopy. Drug release from the nanoparticles was analyzed. RESULTS: The spherical particles produced showed a unimodal and lognormal size distribution, and the geometric number mean size of the nanoparticles could be varied between 90 and 200 nm. When the amount of drug in the polymeric matrix was small, the nanoparticles had a homogeneous, amorphous structure. Drug crystals were formed when the amount of drug was increased over the solubility limit of the drug into the polymer. The amounts of drug and polymer controlled the drug release from the nanoparticles. CONCLUSIONS: The aerosol flow reactor method was found to be able to produce homogeneous amorphous matrix-type nanoparticles that can directly be collected as dry powder.

Aerosols↗