Surface analysis of screwposts.

Abstract

The content and distribution of metallic ions on the surface of gold-plated brass screwposts (Dentatus and MecOdont) were analyzed by X-ray microanalysis. On screwposts from one of the manufacturers the protective outer layer of gold was found to be localized to specific areas of the posts, i.e. the grooves, while unprotected Cu-Zn alloy was found on the ridges. The results are discussed with regard to results on root posts published earlier. Screwposts constructed in this way would appear to be of doubtful clinical value.

Explore related subjects

Keep this discovery

Explore connections, maps & timelines

BibTeXRIS

K Arvidson, R Wróblewski. 1979. Surface analysis of screwposts.. https://doi.org/10.1111/j.1600-0722.1979.tb00667.x

Cite the original work for its findings. Save a collection to share your selection of sources.

KEEP EXPLORING

Related citations

Copper-Containing Surface Engineering for Soft-Tissue Biomedical Devices: Structure-Function Relationships and Ion Release-Driven Biological Performance, A Systematic Review.

Copper and copper-based materials have gained increasing attention for the functional modification of implantable medical devices intended for prolonged soft-tissue contact, including vascular stents, catheters, and intrauterine devices. Owing to their broad-spectrum antimicrobial activity, redox reactivity, and involvement in angiogenesis and cellular signaling, copper-based systems offer significant potential for multifunctional surface engineering. However, achieving a balance between antibacterial efficacy, corrosion behavior, controlled ion release, and cytocompatibility remains a critical challenge. This PRISMA-compliant systematic review analyzes copper-containing materials and surface modification strategies for soft-tissue biomedical applications. A structured search of Scopus, Web of Science, and PubMed (2015-2025) identified 65 eligible studies. The review encompasses bulk copper-containing alloys, electrochemical and chemical surface modification techniques, physical vapor deposition approaches, and advanced hybrid systems integrating copper with polymers, hydrogels, or metal-phenolic networks. Across the reviewed literature, antibacterial performance was strongly dependent on copper concentration, microstructural distribution, and spatiotemporal ion release profiles. Moderate, well-controlled copper incorporation frequently improved antibacterial efficacy while maintaining acceptable hemocompatibility and cytocompatibility, particularly in vascular and blood-contacting devices. In contrast, excessive copper loading often accelerated corrosion and induced adverse cellular responses. Emerging multifunctional architectures demonstrated improved regulation of biological interactions, enabling simultaneous antibacterial, antithrombotic, and proendothelial effects. Overall, copper-based surface technologies represent a versatile platform for soft-tissue implant modification. Future translational progress will require precise control of copper release kinetics and comprehensive long-term in vivo validation to ensure safety and sustained therapeutic performance. From the authors' perspective, the most promising future direction involves multifunctional copper-based hybrid coatings capable of dynamically regulating ion release, host tissue integration, and antibacterial performance simultaneously. Strategies integrating hierarchical architectures, stimulus-responsive release systems, and clinically scalable fabrication methods are expected to play a key role in translating copper-containing surfaces from experimental concepts toward commercially viable soft-tissue biomedical devices.

Copper↗

Development of a new approach for microbial decontamination of water using modified Fenton's reaction.

Microbial decontamination of water was carried out using a novel radical generating system consisting of ion exchange resin, copper and hydrogen peroxide. The system was successful in reducing the microbial load in water by more than 99% in 15 min and is effective against all the microorganisms tested. The method was also successful in decontaminating the flood water obtained from Industrial Canal and 17th Street Canal in New Orleans. Decontamination is due to the formation of hydroxyl radicals, formed during the decomposition of hydrogen peroxide by the metal-polymer complex.

Copper↗