Polyanhydride microsphere formulation by solvent extraction.

Abstract

A novel process based on solvent extraction was developed to produce drug-loaded polyanhydride microspheres for controlled-release applications. The technique consists of adding a chloroform solution of polyanhydride and drug into a stirred silicone oil phase containing suspended droplets of surfactant. No chemical reaction, heating, nor contact with water was required in this process. The microspheres produced were capable of releasing various dyes for prolonged periods of time.

Explore related subjects

Keep this discovery

Explore connections, maps & timelines

BibTeXRIS

C Bindschaedler, K Leong, E Mathiowitz, R Langer. 1988. Polyanhydride microsphere formulation by solvent extraction.. https://doi.org/10.1002/jps.2600770811

Cite the original work for its findings. Save a collection to share your selection of sources.

KEEP EXPLORING

Related citations

Pulsatile protein release from a laminated device comprising polyanhydrides and pH-sensitive complexes.

A laminated device comprising of polyanhydrides as isolating layers and pH-sensitive complexes as protein-loaded layers was designed to deliver proteins in a pulsatile manner. Poly(sebacic anhydride)-b-polyethylene glycol (PSA-b-PEG) and poly(trimellitylimidoglycine-co-sebacic anhydride)-b-polyethylene glycol (P(TMA-gly-co-SA)-b-PEG) were synthesized as isolating layers for their good processing properties at room temperature and suitable erosion duration. During the erosion period, pH of the dissolution fluid decreases to a low value (3.8-5.8). Poly(methacrylic acid)/polyethoxazoline (PMAA/PEOx) complex was used as protein-loaded layers, which could dissociate and release model proteins, Myoglobin (Mb) and Bovine Serum Albumin (BSA), at pH 7.4 while become stable and retained the drugs below pH 5.0. The protein release from the device showed a typical pulsatile fashion. The lag time prior to the pulsatile protein release correlated with the hydrolytic duration of the polyanhydrides, which varied from 30 to 165 h by selecting polyanhydride type and isolating layer thickness. In addition, the pulse duration could be adjusted from 18.5 to 40 h by varying the mass of the complex. The results can be attributed to the synergistic effects between the degrading polyanhydrides, pH-sensitive complexes and proteins.

Anhydrides

Photopolymers in orthopedics: characterization of novel crosslinked polyanhydrides.

Novel, high modulus, degradable polymers were prepared from methacrylated anhydride monomers of tricarballylic acid (MTCA) and pyromellitylimidoalanine (MPMA-ala). Kinetic studies indicate that the time scale of photopolymerization of MTCA (< 30 s) is suitable for in vivo applications. Additionally, the tensile modulus of copolymers of these novel monomers with methacrylic anhydride (MA) ranged from 0.8 to 2.1 GPa, which lies between the modulus of trabecular and cortical bone. Degradation studies indicate that the copolymers of MTCA and MPMA-ala with MA are initially surface degrading, which is important to maintaining polymer strength through the degradation process. Monomers such as these that can be rapidly polymerized using ultraviolet or blue light into high modulus degradable materials have great potential in orthopedics.

Anhydrides