Yarn design for functional tissue engineering.

Tissue engineering requires the ability to design scaffolds with mechanical properties similar to those of the native tissue. Here, B. mori silk yarns are used as a model system to demonstrate the potential benefits and drawbacks of several textile methods used to fabricate tissue engineering scaffolds. Fibers are plied, twisted, cabled, braided, and/or textured to form several geometries with a wide range of mechanical outcomes. Predictable changes in ultimate tensile strength and stiffness are demonstrated following processing and as a function of test environment. The mechanical effects of increasing turns per inch and combining groups of fibers into higher-order yarn structures are demonstrated. Braids, one of the most commonly used textile structures, are shown to be limited by a change in stiffness following the locking-angle and therefore, potentially not the ideal structure for tissue engineering. Cabled yarns appear to allow the most flexibility in mechanical outcomes with a highly organized geometry. Twisted yarns, while more economical than cabled yarns, result in a higher stiffness and lower percent elongation at break than cabled yarns.

Animals↗

In vitro degradation of silk fibroin.

A significant need exists for long-term degradable biomaterials which can slowly and predictably transfer a load-bearing burden to developing biological tissue. In this study Bombyx mori silk fibroin yarns were incubated in 1mg/ml Protease XIV at 37 degrees C to create an in vitro model system of proteolytic degradation. Samples were harvested at designated time points up to 12 weeks and (1) prepared for scanning electron microscopy (SEM), (2) lyophilized and weighed, (3) mechanical properties determined using a servohydraulic Instron 8511, (4) dissolved and run on a SDS-PAGE gel, and (5) characterized with Fourier transform infrared spectroscopy. Control samples were incubated in phosphate-buffered saline. Fibroin was shown to proteolytically degrade with predictable rates of change in fibroin diameter, failure strength, cycles to failure, and mass. SEM indicated increasing fragmentation of individual fibroin filaments from protease-digested samples with time of exposure to the enzyme; particulate debris was present within 7 days of incubation. Gel electrophoresis indicated a decreasing amount of the silk 25 kDa light chain and a shift in the molecular weight of the heavy chain with increasing incubation time in protease. Results support that silk is a mechanically robust biomaterial with predictable long-term degradation characteristics.

Absorbable Implants↗

Silk-based biomaterials.

Silk from the silkworm, Bombyx mori, has been used as biomedical suture material for centuries. The unique mechanical properties of these fibers provided important clinical repair options for many applications. During the past 20 years, some biocompatibility problems have been reported for silkworm silk; however, contamination from residual sericin (glue-like proteins) was the likely cause. More recent studies with well-defined silkworm silk fibers and films suggest that the core silk fibroin fibers exhibit comparable biocompatibility in vitro and in vivo with other commonly used biomaterials such as polylactic acid and collagen. Furthermore, the unique mechanical properties of the silk fibers, the diversity of side chain chemistries for 'decoration' with growth and adhesion factors, and the ability to genetically tailor the protein provide additional rationale for the exploration of this family of fibrous proteins for biomaterial applications. For example, in designing scaffolds for tissue engineering these properties are particularly relevant and recent results with bone and ligament formation in vitro support the potential role for this biomaterial in future applications. To date, studies with silks to address biomaterial and matrix scaffold needs have focused on silkworm silk. With the diversity of silk-like fibrous proteins from spiders and insects, a range of native or bioengineered variants can be expected for application to a diverse set of clinical needs.

Animals↗

Silk matrix for tissue engineered anterior cruciate ligaments.

A silk-fiber matrix was studied as a suitable material for tissue engineering anterior cruciate ligaments (ACL). The matrix was successfully designed to match the complex and demanding mechanical requirements of a native human ACL, including adequate fatigue performance. This protein matrix supported the attachment, expansion and differentiation of adult human progenitor bone marrow stromal cells based on scanning electron microscopy, DNA quantitation and the expression of collagen types I and III and tenascin-C markers. The results support the conclusion that properly prepared silkworm fiber matrices, aside from providing unique benefits in terms of mechanical properties as well as biocompatibility and slow degradability, can provide suitable biomaterial matrices for the support of adult stem cell differentiation toward ligament lineages. These results point toward this matrix as a new option for ACL repair to overcome current limitations with synthetic and other degradable materials.

Animals↗

Advanced bioreactor with controlled application of multi-dimensional strain for tissue engineering.

Advanced bioreactors are essential for meeting the complex requirements of in vitro engineering functional skeletal tissues. To address this need, we have developed a computer controlled bench-top bioreactor system with capability to apply complex concurrent mechanical strains to three-dimensional matrices independently housed in 24 reactor vessels, in conjunction with enhanced environmental and fluidic control. We demonstrate the potential of this new system to address needs in tissue engineering, specifically toward the development of a tissue engineered anterior cruciate ligament from human bone-marrow stromal cells (hBMSC), where complex mechanical and biochemical environment control is essential to tissue function. Well-controlled mechanical strains (resolution of < 0.1 micron for translational and < 0.1 degree for rotational strain) and dissolved oxygen tension (between 0%-95% +/- 1%) could be applied to the developing tissue, while maintaining temperature at 37 +/- 0.2 degrees C about developing tissue over prolonged periods of operation. A total of 48 reactor vessels containing cell culture medium and silk fiber matrices were run for up to 21 days under 90 degrees rotational and 2 mm translational deformations at 0.0167 Hz with only one succumbing to contamination due to a leak at an medium outlet port. Twenty-four silk fiber matrices seeded with human bone marrow stromal cells (hBMSCs) housed within reactor vessels were maintained at constant temperature (37 +/- 0.2 degrees C), pH (7.4 +/- 0.02), and pO2 (20 +/- 0.5%) over 14 days in culture. The system supported cell spreading and growth on the silk fiber matrices based on SEM characterization, as well as the differentiation of the cells into ligament-like cells and tissue (Altman et al., 2001).

Biomimetics↗

Cell differentiation by mechanical stress.

Growth factors, hormones, and other regulatory molecules are traditionally required in tissue engineering studies to direct the differentiation of progenitor cells along specific lineages. We demonstrate that mechanical stimulation in vitro, without ligament-selective exogenous growth and differentiation factors, induces the differentiation of mesenchymal progenitor cells from the bone marrow into a ligament cell lineage in preference to alternative paths (i.e., bone or cartilage cell lineages). A bioreactor was designed to permit the controlled application of ligament-like multidimensional mechanical strains (translational and rotational strain) to the undifferentiated cells embedded in a collagen gel. The application of mechanical stress over a period of 21 days up-regulated ligament fibroblast markers, including collagen types I and III and tenascin-C, fostered statistically significant cell alignment and density and resulted in the formation of oriented collagen fibers, all features characteristic of ligament cells. At the same time, no up-regulation of bone or cartilage-specific cell markers was observed.

Animals↗

Sequential growth factor application in bone marrow stromal cell ligament engineering.

In vitro bone marrow stromal cell (BMSC) growth may be enhanced through culture medium supplementation, mimicking the biochemical environment in which cells optimally proliferate and differentiate. We hypothesize that the sequential administration of growth factors to first proliferate and then differentiate BMSCs cultured on silk fiber matrices will support the enhanced development of ligament tissue in vitro. Confluent second passage (P2) BMSCs obtained from purified bone marrow aspirates were seeded on RGD-modified silk matrices. Seeded matrices were divided into three groups for 5 days of static culture, with medium supplement of basic fibroblast growth factor (B) (1 ng/mL), epidermal growth factor (E; 1 ng/mL), or growth factor-free control (C). After day 5, medium supplementation was changed to transforming growth factor-beta1 (T; 5 ng/mL) or C for an additional 9 days of culture. Real-time RT-PCR, SEM, MTT, histology, and ELISA for collagen type I of all sample groups were performed. Results indicated that BT supported the greatest cell ingrowth after 14 days of culture in addition to the greatest cumulative collagen type I expression measured by ELISA. Sequential growth factor application promoted significant increases in collagen type I transcript expression from day 5 of culture to day 14, for five of six groups tested. All T-supplemented samples surpassed their respective control samples in both cell ingrowth and collagen deposition. All samples supported spindle-shaped, fibroblast cell morphology, aligning with the direction of silk fibers. These findings indicate significant in vitro ligament development after only 14 days of culture when using a sequential growth factor approach.