Osteopontin-hydroxyapatite interactions in vitro: inhibition of hydroxyapatite formation and growth in a gelatin-gel.

Osteopontin is a phosphorylated bone matrix sialoprotein, postulated to play a regulatory role in biomineralization. The effects of a crude preparation of rat bone osteopontin and a more highly purified bovine bone osteopontin were evaluated using a gel diffusion system to measure effects of 0.1-100 micrograms/ml of this matrix protein on hydroxyapatite formation and crystal proliferation. Bovine osteopontin at concentrations greater than 25 micrograms/ml inhibited both hydroxyapatite formation and growth in a dose-dependent manner. Osteopontin at concentrations lower than 25 micrograms/ml had no detectable effect on the amount of mineral accumulated in experiments with and without pre-formed hydroxyapatite seed crystals either when initial mineral deposition was assessed at 3.5 days, or when mineral formation and growth were assessed at 5 days. There was a statistically significant dose-dependent decrease in crystal length at all concentrations tested. The rat osteopontin preparation had similar inhibitory abilities. Partial dephosphorylation of bovine osteopontin with alkaline phosphatase removed its inhibitory ability, and reduced its ability to bind calcium. The affinity of bovine osteopontin for hydroxyapatite was determined based on a Langmuir adsorption isotherm, with values of K (binding affinity) and N (number of binding sites) being 0.026 ml/microgram and 1084 micrograms/m2, respectively. The data suggest that, in this system, osteopontin is an effective inhibitor of hydroxyapatite formation and growth due to its affinity for the hydroxyapatite crystals. In this system, osteopontin, distinct from other phosphoproteins which both promote and inhibit hydroxyapatite deposition, did not enhance mineral formation at any concentration tested.

Animals↗

Articular cartilage vesicles generate calcium pyrophosphate dihydrate-like crystals in vitro.

OBJECTIVE: To identify the morphology of a mineral-forming of adult porcine hyaline articular cartilage digest and characterize the mineral it forms. METHODS: Electron microscopy, Fourier transform infrared (FTIR) spectroscopy, x-ray microanalysis, compensated polarized light microscopy, and biochemical studies including 14C-labeled UDPG pyrophosphohydrolase radiometric assay. RESULTS: This fraction of articular cartilage digest contained membrane-limited vesicles resembling growth plate cartilage matrix vesicles and formed mineral after only 24 hours in physiologic salt solution containing 1 mM ATP: The mineral contained inorganic pyrophosphate, 95% of which derived from ATP, and phosphate, 93% of which derived from inorganic phosphate in the medium. The FTIR spectrum of this mineral closely resembled the spectrum of standard calcium pyrophosphate dihydrate (CPPD) crystals. Compensated polarized light microscopy showed positively birefringent, rod-shaped crystals morphologically identical to CPPD. Ca:P ratios, defined by energy-dispersive microanalysis, were also consistent with CPPD. CONCLUSION: The articular cartilage vesicle fraction of porcine hyaline cartilage is capable of generating mineral that strongly resembles CPPD.

Adenosine Triphosphate↗

Treatment of proteoglycan aggregates with physeal enzymes reduces their ability to inhibit hydroxyapatite proliferation in a gelatin gel.

In vitro, cartilage proteoglycans (PGs) are effective inhibitors of hydroxyapatite formation and growth. Their inhibitory ability decreases with decreasing PG size and charge density. It has been suggested that the enzyme-mediated alteration in the size and conformation of PGs in the growth plate may similarly facilitate the calcification process. In this study, a gelatin gel system was used to monitor hydroxyapatite formation and growth in the presence of proteoglycan aggregates, before and after enzyme treatment. To reproduce the physeal degradation cascade, an enzyme preparation was used that contained all of the growth plate enzymes. At a concentration of 500 micrograms/ml, the untreated proteoglycan aggregates reduced the amount of mineral formed by 30%. When the aggregates were treated with the heat-inactivated enzyme, the same extent of inhibition was found. In contrast, treating the aggregates with the crude growth plate enzyme preparation removed all the inhibitory ability, such that 500 micrograms/ml of proteoglycan preparation yielded 10% more mineral than the controls. Treatment of the aggregates with chondroitinase ABC and trypsin, similarly removed all the inhibitory ability. These data, suggest that enzymatic degradation of proteoglycans may contribute to the regulation of growth plate calcification.

Animals↗

Effect of short-term hypomagnesemia on the chemical and mechanical properties of rat bone.

Magnesium is known to have an essential role in determining the properties of bone, but the way in which Mg exerts its actions remains unclear. Although long-term Mg deficiency is known to produce osteopenia, the effects of short-term Mg deficiency have not been established. To test the hypothesis that Mg deficiency results in an altered pattern of initial mineralization and concomitant altered bone properties, the radiographic, histologic, chemical, and mechanical properties of the bones of rats given a Mg-deficient diet were compared to those of rats pair-fed the same diet supplemented with Mg. Short-term Mg-deficiency in the diet of growing rats produced a significant decrease in both the trabecular bone volume and the mineral content of the newly formed metaphysis, a significant increase in the Ca:P ratio, and a slight, but significant increase in hydroxyapatite crystallite size and/or perfection in the metaphysis. Comparable, but not significant, trends were found in the diaphyses. Metaphyseal bone osteocalcin levels were reduced in the Mg-deficient rats and lipid was more easily extracted from their bones. No detectable alterations in radiographic microstructure were noted. Mechanically, a significant decrease in the maximum three-point bend strength of the femurs of Mg-deficient rats was observed. These data support the hypothesis that short-term Mg deficiency affects the pattern of bone mineral formation.

Animals↗

An FT-IR microscopic investigation of the effects of tissue preservation on bone.

Fourier transform infrared microscopy is a powerful tool for the characterization of mineral and protein in histologic sections of bone. This study was concerned with determining whether techniques used to preserve these tissues and to prepare them for sectioning had an effect on spectral properties. The nu 1, nu 3 phosphate bands in the 900-1200 cm-1 spectral region were used to evaluate the structure of the apatitic mineral in fresh-frozen, ethanol-fixed, and formalin-fixed 35-day-old rat femurs; fresh-frozen and formalin-fixed 20-day-old fetal rat femurs; ground 35-day-old rat diaphyseal bone samples; and formalin-fixed, methacrylate-embedded ground diaphyseal bone. The crystallinity (crystal size and perfection) of the bone apatite was assessed by a curve-fitting analysis of the nu 1, nu 3 phosphate bands. Results indicate that ethanol or formalin fixation of the 35-day-old intact rat femur, and formalin fixation and embedding of the ground rat bone do not significantly alter the crystallinity of the apatite. However, formalin fixation of the fetal rat bone did alter the structure of the apatite mineral phase. In addition, evaluation of protein secondary structure in the 35-day-old rat femur from the Amide I and Amide II vibrations near 1650 and 1550 cm-1, respectively, revealed that protein conformation was altered by ethanol fixation.

Amides↗

FT-IR microscopic mappings of early mineralization in chick limb bud mesenchymal cell cultures.

Chick limb bud mesenchymal cells differentiate into chondrocytes and form a cartilaginous matrix in culture. In this study, the mineral formed in different areas within cultures supplemented with 4 mM inorganic phosphate, or 2.5, 5.0, and 10 mM beta-glycerophosphate (beta GP), was characterized by Fourier-transform infrared (FT-IR) microscopy. The relative mineral-to-matrix ratios, and distribution of crystal sizes at specific locations throughout the matrix were measured from day 14 to day 30. The only mineral phase detected was a poorly crystalline apatite. Cultures receiving 4 mM inorganic phosphate had smaller crystals which were less randomly distributed around the cartilage nodules than those in the beta GP-treated cultures. beta GP-induced mineral consisted of larger, more perfect apatite crystals. In cultures receiving 5 or 10 mM beta GP, the relative mineral-to-matrix ratios (calculated from the integrated intensities of the phosphate and amide I bands, respectively) were higher than in the cultures with 4 mM inorganic phosphate or in the in vivo calcified chick cartilage.

Animals↗

Studies of matrix vesicle-induced mineralization in a gelatin gel.

Matrix vesicles isolated from fourth-passage cultures of chondrocytes were tested for their ability to induce hydroxyapatite formation in a gelatin gel in order to gain insight into the function of matrix vesicles in in situ mineralization. These matrix vesicles did not appear to be hydroxyapatite nucleators per se since the extent of mineral accumulation in the gel diffusion system was not altered by the presence of matrix vesicles alone, and in the vesicle containing gels, mineral crystals were formed whether associated with vesicles or not. In gels with these matrix vesicles and beta-glycerophosphate, despite the presence of alkaline phosphatase activity, there was no increase in mineral deposition. This suggested that in the gel system these culture-derived vesicles did not increase local phosphate concentrations. However, when known inhibitors of mineral crystal formation and growth (proteoglycan aggregates [4 mg/ml], or ATP [1 mM], or both proteoglycan and ATP) were included in the gel, more mineral was deposited in gels with the vesicles than in comparable gels without vesicles, indicating that enzymes within these vesicles were functioning to remove the inhibition. These data support the suggestion that one function of the extracellular matrix vesicles is to transport enzymes for matrix modification.

Adenosine Triphosphate↗

Studies of mineralization in tissue culture: optimal conditions for cartilage calcification.

The optimal conditions for obtaining a calcified cartilage matrix approximating that which exists in situ were established in a differentiating chick limb bud mesenchymal cell culture system. Using cells from stage 21-24 embryos in a micro-mass culture, at an optimal density of 0.5 million cells/20 microliters spot, the deposition of small crystals of hydroxyapatite on a collagenous matrix and matrix vesicles was detected by day 21 using X-ray diffraction, FT-IR microscopy, and electron microscopy. Optimal media, containing 1.1 mM Ca, 4 mM P, 25 micrograms/ml vitamin C, 0.3 mg/ml glutamine, no Hepes buffer, and 10% fetal bovine serum, produced matrix resembling the calcifying cartilage matrix of fetal chick long bones. Interestingly, higher concentrations of fetal bovine serum had an inhibitory effect on calcification. The cartilage phenotype was confirmed based on the cellular expression of cartilage collagen and proteoglycan mRNAs, the presence of type II and type X collagen, and cartilage type proteoglycan at the light microscopic level, and the presence of chondrocytes and matrix vesicles at the EM level. The system is proposed as a model for evaluating the events in cell mediated cartilage calcification.

Aggrecans↗

Matrix mineralization in hypertrophic chondrocyte cultures. Beta glycerophosphate increases type X collagen messenger RNA and the specific activity of pp60c-src kinase.

The phenomenon of chondrocyte hypertrophy is accompanied by the expression of type X collagen and the appearance of matrix mineralization. These events are also associated with changes in the phosphorylation of intracellular proteins. In this study the addition of 10 mM beta-glycerophosphate to hypertrophic chondrocytes resulted in stimulation of type X collagen synthesis up to 10 days in culture and an increase in the expression of type X collagen mRNA. This was followed by the onset of mineralization and the appearance of calcium hydroxyapatite. In contrast, the addition of beta-glycerophosphate to non-hypertrophic chondrocytes failed to induce expression of type X collagen or to produce changes in calcium and phosphate. The increased formation of type X collagen and of mineral in hypertrophic chondrocytes was accompanied by changes in the tyrosine kinase pp60c-src. While the level of c-src protein decreased approximately 2.5-fold in hypertrophic chondrocytes after 17 days of beta-glycerophosphate treatment, the specific activity of pp60c-src kinase increased approximately 3-fold in the cells that could be induced to mineralize but remained unchanged in cells that did not exhibit this property. Regulation of kinase activity may be an important event in endochondral ossification.

Animals↗

An infrared study of the interaction of polymethyl methacrylate with the protein and mineral components of bone.

We used Fourier transform infrared (FT-IR) microscopic mapping techniques to investigate the infiltration of polymethyl methacrylate (PMMA), a widely used medium for embedding biological tissues, into rat femur sections. Monitoring of the infrared absorbances of the PMMA carbonyl stretch, the protein amide I, and the apatite mineral phosphate stretch over a 225 x 975-microns region of the epiphyseal growth plate region of the rat femur enabled comparison of the relative amount of each component in distinct regions of the tissue. It was found that PMMA penetrates less into regions of greater mineral density and that the frequency of the PMMA carbonyl absorbance from the embedded tissue, 1729 cm-1, is identical to the free PMMA carbonyl frequency. This is consistent with a diffusion mechanism of infiltration of the PMMA, with no specific chemical interaction between the PMMA and the tissue components.

Animals↗

Mineral-matrix interactions in bone and cartilage.

Mineral-matrix interactions regulate the process of hydroxyapatite formation in bones and teeth. In mineralizing tissues, many anionic macromolecules bind to mineral. By means of this binding, such molecules are able to regulate the size and shape of the mineral crystals, determine the site of initial crystal deposition, and determine the type of mineral crystals deposited. Collagen, which provides a template for hydroxyapatite deposition; extracellular matrix vesicles, which provide a protected environment for crystal deposition; and noncollagenous matrix proteins that have high affinities for hydroxyapatite have all been shown to affect mineralization in vitro. Some of the noncollagenous proteins have been shown to be capable of promoting and inhibiting mineral formation and growth, depending on their concentration and whether they are immobilized or free in solution. This review surveys the current understanding of mineral-matrix relationships involved in endochondral, intramembranous, and appositional bone formation, outlining the way in which mineral deposition is controlled in mammalian calcified tissues. The structural basis for the interaction of the matrix molecules with hydroxyapatite is presented, as is the in vitro and in situ data implicating the matrix molecules that interact with hydroxyapatite to control mineralization.

Bone Matrix↗

Effects of propranolol on bone metabolism in the rat.

Propranolol, a nonspecific beta-blocker has many physiologic effects. Its effects on bone in vivo are unknown, although beta receptor sites have been found on osteoblasts. In this study, the hypothesis tested was that low doses of propranolol could alter bone properties and enhance orthotopic endochondral bone formation. In a group of nonsurgical rats, propranolol treatment increased femoral torsional strength on biomechanical testing. In the rat surgical model used, right femora were fixed to a polyethylene plate and then defects were created mid-diaphysis and subsequently filled with demineralized bone matrix. These rats (defect rats) were randomly divided into groups that were given propranolol or a saline carrier for 19 consecutive days. In the defect rats, increased trabecular femoral metaphyseal mineral apposition rates were observed in propranolol-treated groups. Densitometry and roentgenographic scoring of callus formation after 12 weeks in propranolol-treated rats revealed increased callus and bone union. The results of this study indicate that propranolol treatment can significantly affect bone properties.

Animals↗

Hydroxyapatite formation in the presence of proteoglycans of reduced sulfate content: studies in the brachymorphic mouse.

Proteoglycans from the brachymorphic (bm/bm) mouse have a reduced sulfate content due to the impaired activity of adenosine phosphosulfate phosphokinase in these animals. X-ray diffraction and infrared analyses of the mineral from the calcified cartilage of the bm/bm mice demonstrate the presence of significantly larger and more perfect hydroxyapatite crystals of lower carbonate to phosphate content than crystals found in the control animals. No differences were seen in the mineral content, crystallite size, CO3:PO4 ratio, or infrared splitting factors measured in the diaphyseal bone from these animals. Electron microscopic examination similarly shows larger, more disorganized crystals in the bm/bm animals' calcified cartilage as contrasted with controls. In vitro, proteoglycan aggregates from these dwarf mice are shown in a collagen gel-growth system to be less effective inhibitors of hydroxyapatite formation and growth than similarly size sulfated proteoglycans from age-matched control animals. The proteoglycans from the control mice were comparable in inhibitory ability to proteoglycan aggregates extracted from fetal bovine epiphyses. The in vitro and in vivo mineral parameters suggest the importance of sulfate for the interaction between proteoglycans and mineral in growth plate calcification.

Animals↗

The effect of phosphatidylserine on in vitro hydroxyapatite growth and proliferation.

The acidic phospholipid phosphatidylserine (PS) has been reported to have variable effects on in vitro hydroxyapatite proliferation. PS promotes in vitro mineralization in systems in which calcium-PS-phosphate complexes are allowed to form, and inhibits in vitro mineralization when incorporated into liposomes. To investigate these diverse effects, a Langmuir adsorption isotherm was used to determine the affinity of PS for hydroxyapatite crystals, based on binding of 14C-PS to synthetic hydroxyapatite crystals of specific surface 54 m2/g. Using this model, PS was found to bind to hydroxyapatite crystals with an affinity comparable to that of the amino acid phosphoserine (K = 3.33 ml/mumol). Coating the surface of hydroxyapatite seed crystals with PS reduced their rate of proliferation in a metastable calcium phosphate solution in which calcium-PS-phosphate complexes were previously shown to promote hydroxyapatite formation. The extent of inhibition of hydroxyapatite seeded growth was directly related to the proportion of the hydroxyapatite surface covered with PS. These data suggest that PS may have multiple effects on hydroxyapatite formation in situ, and that mineral-PS interactions can retard crystal proliferation.

Calcium Phosphates↗

Bone particles from gallium-treated rats are resistant to resorption in vivo.

Gallium nitrate is a clinically effective agent for the treatment of cancer related hypercalcemia. The mechanism of action of this agent was investigated following development of a quantitative in vivo bone resorption assay modified from the method of Glowacki. In a preliminary study, the time course of resorption of 50 mg subcutaneous implants of bone powder in growing rats was followed by chemical analysis of mineral (ash and Ca) contents, enzymatic and histochemical assay of tartrate resistant acid phosphatase (TRAP) activity, and image analysis of changes in particle size using von Kossa stained sections. Day 21 was chosen as a single time point for the comparison of the extent of resorption of gallium-containing and control bone particles. Resorption of bone particles containing 0.39 micrograms Ga/mg bone was significantly inhibited relative to control particles. Mineral content (6.7 vs. 3.6 mg), Ca content (1.72 vs. 1.37 mg), and the percentage of the field covered by bone particles (12 vs. 9%) were greater in the animals which received gallium-containing bone particles. Similarly, the number of osteoclast-like cells and the TRAP activity in the gallium-containing bone particle implants at 21 days were increased relative to controls. These data indicate that gallium incorporation into bone matrix confers resistance to resorption.

Acid Phosphatase↗

Phospholipid changes in the bones of the hypophosphatemic mouse.

The mineral and lipid composition of the bones of 35 day old hypophosphatemic (Hyp/Y) and control (+/Y) mice were compared in order to test the hypothesis that phosphate status has an effect on the complexed acidic phospholipid content of developing bones. The Hyp/Y bones were found to be rachitic and osteomalacic, having significantly reduced mineral content. That mineral was shown by X-ray diffraction to consist of larger/more perfect crystals than that in +/Y animals, indicating either a preference for crystal growth rather than new mineral deposition, or an increased mineral turnover. The increased crystal perfection was confirmed by chemical analyses which showed an increased calcium to phosphorus ratio in the Hyp/Y bones. The bones of Hyp/Y animals had significantly reduced complexed acidic phospholipid contents relative to those of control animals. Since these complexes are believed to play a role in vitro and in vivo mineral deposition, it is suggested that the deficiency of these complexes contributes to the mineralization defect. The magnitude of the complexed acidic phospholipid deficiency in the Hyp/Y animals indicates the importance of phosphate for the formation of these lipids. Although the proportion of phosphatidylserine and phosphatidylinositol and lysophospholipids tended to be reduced in the Hyp/Y bones, the absence of other statistically significant phospholipid abnormalities in the bones and brains of these animals suggests that the lipid defect is not systemic, but is associated with a decrease in phosphate at the site of bone formation.

Animals↗

Requirement of vitamin C for cartilage calcification in a differentiating chick limb-bud mesenchymal cell culture.

Mesenchymal cells isolated from stage 21-24 chick limb-buds plated in a micro-mass culture differentiate to form chondrocytes and synthesize a calcifiable matrix. In the presence of inorganic phosphate (4 mM), hydroxyapatite mineral deposits around cartilage nodules. Ascorbic acid is, in general, an essential co-factor for extracellular matrix synthesis in culture, since it is required for collagen synthesis. In this study we demonstrate that in the absence of ascorbic acid supplementation in the mesenchymal cell cultures, mineral deposition (indicated by X-ray diffraction, measurement of Ca:hydroxyproline ratio, and 45Ca uptake) does not occur. Concentrations of 10-50 micrograms/ml ascorbate were compared to find the "optimal" concentration for cell mediated mineralization; 25 micrograms/ml was selected as optimal based on matrix appearance at the EM level and the rate of 45Ca uptake. High concentrations of ascorbic acid (greater than 75 micrograms/ml), while increasing the amount of hydroxyproline in the matrix synthesized, caused some cell death and hence less cell-mediated mineralization. This study demonstrates both the need for viable cells and a proper matrix for in vitro cell-mediated mineralization, and shows that varying the concentration of L-ascorbate (vitamin C) in the medium can have a marked effect on mineralization in vitro.

Alkaline Phosphatase↗

Hyaluronan interactions with hydroxyapatite do not alter in vitro hydroxyapatite crystal proliferation and growth.

The interaction of hyaluronan (Mr range 80-120 x 10(4)) with poorly crystalline hydroxyapatite, such as is found in calcified cartilage and bone, was studied to challenge the hypothesis that free hyaluronan found in proteoglycan aggregate preparations could affect in vitro mineralization. Using a Langmuir adsorption isotherm, based on uronic acid content, hyaluronan was found to bind to hydroxyapatite with an affinity K of 0.12 ml/microgram uronate and N = 6.8 micrograms uronate/m2 hydroxyapatite binding sites. This is contrasted with K = .047 ml/microgram uronate and N = 9.0 micrograms uronate/m2 for a bovine nasal proteoglycan monomer preparation. Although the proteoglycan monomer and aggregate preparations have been reported to inhibit hydroxyapatite growth at concentrations of 1 mg/ml, using solution concentrations of 0, 0.01, 0.1 and 1 mg/ml hyaluronan there were no detectable alterations in the rate of seeded hydroxyapatite growth and proliferation. These data indicate that although in vitro hyaluronan may bind with weak affinity to hydroxyapatite, this interaction does not affect mineral growth, and the presence of hyaluronan would not contribute to the increased inhibitory potential of cartilage proteoglycan aggregate relative to monomer preparations.

Adsorption↗