Search PubMed⌕ Search

Biomedical subjects

A Della Bona

Publications and source records attributed to A Della Bona.

10 recordsLinked to original sources

Apparent interfacial fracture toughness of resin/ceramic systems.

We suggest that the apparent interfacial fracture toughness (K(A)) may be estimated by fracture mechanics and fractography. This study tested the hypothesis that the K(A) of the adhesion zone of resin/ceramic systems is affected by the ceramic microstructure. Lithia disilicate-based (Empress2-E2) and leucite-based (Empress-E1) ceramics were surface-treated with hydrofluoric acid (HF) and/or silane (S), followed by an adhesive resin. Microtensile test specimens (n = 30; area of 1 +/- 0.01 mm(2)) were indented (9.8 N) at the interface and loaded to failure in tension. We used tensile strength (sigma) and the critical crack size (c) to calculate K(A) (K(A) = Ysigmac(1/2)) (Y = 1.65). ANOVA and Weibull analyses were used for statistical analyses. Mean K(A) (MPa.m(1/2)) values were: (E1HF) 0.26 +/- 0.06; (E1S) 0.23 +/- 0.06; (E1HFS) 0.30 +/- 0.06; (E2HF) 0.31 +/- 0.06; (E2S) 0.13 +/- 0.05; and (E2HFS) 0.41 +/- 0.07. All fractures originated from indentation sites. Estimation of interfacial toughness was feasible by fracture mechanics and fractography. The K(A) for the systems tested was affected by the ceramic microstructure and surface treatment.

Acid Etching, Dental↗

Comparative in vivo analysis of the sealing ability of three endodontic sealers in post-prepared root canals.

AIM: To compare the sealing ability of the endodontic sealers AH Plus, Sealer 26 and Endofill in premolar teeth of dogs exposed to the oral cavity after post-preparation. METHODOLOGY: Forty teeth with two canals each underwent root canal cleaning and shaping. Before filling, the canals were randomly distributed into three groups according to the sealer to be used: Group 1 - AH Plus; Group 2 - Sealer 26; and Group 3 - Endofill (Dentsply, Indústria e Comércio Ltda.). Immediately after filling, the gutta percha and sealer were partially removed from the canals, leaving material only in the apical third of the root. The teeth were temporarily sealed with glass ionomer sealer for 72 h to ensure setting. The coronal seal was then removed and the canals were exposed to the oral cavity for 45 days. The animals were euthanased and their mandibles and maxillae were removed. After abundant irrigation with distilled water, the canals were dried and filled with India ink. The teeth were sealed again for 96 h before extraction. The roots of the extracted premolars were separated and stored in labelled test tubes. The roots were cleared and the extent of dye penetration was measured with a 20x stereoscopic magnifying lens. RESULTS: Statistical analysis revealed that there were significant differences between the sealers studied (P < 0.001). Means for the extent of dye penetration for AH Plus, Endofill and Sealer 26 were, respectively, 0.13, 2.27 and 3.08 mm. CONCLUSIONS: After 45 days exposure to the oral cavity, none of the sealers was capable of preventing leakage and coronal dye penetration. There were significant differences between the sealers studied, in terms of mean dye penetration.

Analysis of Variance↗

Microtensile strength of composite bonded to hot-pressed ceramics.

PURPOSE: The objective of this in vitro study employing the microtensile test was to test the hypothesis that the tensile bond strength of hot-pressed ceramics to composite is controlled by the ceramic microstructure and the ceramic surface treatment. MATERIALS AND METHODS: Hot-pressed IPS Empress (E1) and IPS Empress 2 (E2) ceramic blocks were polished with 1-micron alumina abrasive and treated as follows: group 1: 9.6% hydrofluoric acid (HF) on E1; group 2: 4% acidulated phosphate fluoride (APF) on E1; group 3: silane (S) on E1; group 4: HF + S on E1; group 5: APF + S on E1; group 6: HF on E2; group 7: APF on E2; group 8: S on E2; group 9: HF + S on E2; group 10: APF + S on E2. The surfaces as described above were then treated with Scotchbond Multi-Purpose Plus and covered with composite (Z-100). From the blocks obtained in this manner, specimens for microtensile testing were created by sectioning. Twenty bar specimens for each group were loaded to failure under tension using an Instron testing machine. RESULTS: Mean tensile bond strength (MPa) and standard deviation values are as follows: (1) 9.9 +/- 1.2; (2) 0; (3) 27.2 +/- 4.8; (4) 20.6 +/- 3.0; (5) 13.6 +/- 4.5; (6) 41.7 +/- 6.7; (7) 19.1 +/- 2.6; (8) 30.1 +/- 5.3; (9) 56.1 +/- 4.1; (10) 36.9 +/- 3.9. All fractures occurred within the adhesion zone. SEM images of chemically etched specimens revealed that HF produced greater surface degradation and greater bond strength than APF for both E1 and E2 ceramics. The mean bond strength of groups 6 through 10 (E2) was significantly greater than that of groups 1 through 5 (E1) for each treatment condition. CONCLUSION: The tensile fracture resistance of the composite-ceramic adhesion zones is controlled primarily by ceramic microstructure and ceramic surface treatment.

Acid Etching, Dental↗

Ceramic surface preparations for resin bonding.

PURPOSE: To evaluate the effects of hydrofluoric acid (HF) and acidulated phosphate fluoride (APF) primers on differently prepared leucite-containing feldspar ceramic surfaces. MATERIALS AND METHODS: Discs of a leucite-containing feldspar ceramic were prepared following the manufacturer's instructions. Surfaces were either polished, grit blasted or prepared with a diamond bur and then subjected to a range of etching procedures using HF or APF. The surface topography was examined using scanning electron microscopy (SEM). Back-scattered imaging, EDS and X-ray diffraction (XRD) were used for microstructural and compositional analysis. RESULTS: The etching process with HF consisted of a preferential attack of the leucite phase relative to the glass but also removed all features of the previous surface preparation. In contrast, APF etching resulted in the formation of surface deposits, superimposed on the surface roughness created by the prior surface preparations. It was not possible to identify the deposits after APF etching using XRD.

Acid Etching, Dental↗

The effect of amalgam bonding on resistance form of Class II amalgam restorations.

OBJECTIVE: This study evaluated the load required to produce failure in Class II bonded amalgam restorations. METHOD AND MATERIALS: Five groups of 12 maxillary molars were mounted. Class II mesio-occlusal preparations were cut: group 1, extension through central grooves, without retention grooves; group 2, proximal slot preparation, without retention grooves; groups 3 and 5, slot preparation with long facial and lingual retention grooves; group 4, slot preparation without grooves, with unsupported proximal enamel allowed to remain. Groups 1 to 4 were restored with an amalgam-bonding system and amalgam; in group 5, no amalgam-bonding material was used. RESULTS: Mean (SD) failure loads: group 1, 281 (77) N; group 2, 246 (101) N; group 3, 238 (84) N; group 4, 254 (100) N; and group 5, 191 (66) N. CONCLUSION: Although there was a trend toward greater resistance to dislodgment or fracture when an amalgam-bonding technique was used, its use did not significantly increase the resistance to failure when compared to retention grooves alone.

Analysis of Variance↗

Shear vs. tensile bond strength of resin composite bonded to ceramic.

Since the mode of failure of resin composites bonded to ceramics has frequently been reported to be cohesive fracture of either ceramic or resin composite rather than separation at the adhesive interface, this study was designed to question the validity of shear bond strength tests. The reasons for such a failure mode are identified and an alternative tensile bond strength test evaluated. Three configurations (A, conventional; B, reversed; and C, all composite) of the cylinder-on-disc design were produced for shear bond strength testing. Two-dimensional finite element stress analysis (FEA) was carried out to determine qualitatively the stress distribution for the three configurations. A tensile bond strength test was designed and used to evaluate two ceramic repair systems, one using hydrofluoric acid (HF) and the other acidulated phosphate fluoride (APF). Results from the shear bond strength tests and FEA showed that this particular test has as its inherent feature the measurement of the strength of the base material rather than the strength of the adhesive interface. In the tensile test, failure invariably occurred in the adhesive layer, with HF and APF showing a similar ability to improve the bond of resin composite to ceramic. It is concluded that the tensile bond strength test is more appropriate for evaluating the adhesive capabilities of resin composites to ceramics.

Acidulated Phosphate Fluoride↗

Shear bond strength of resin bonded ceramic after different try-in procedures.

Final cementation of porcelain laminate veneers may require a previous colour match try-in. The purpose of this in vitro study was to evaluate the effect on shear bond strength of resin bonded to porcelain after the application of different try-in procedures. Forty porcelain specimens were fabricated, flattened with 600 grit SiC, etched with hydrofluoric acid and silane treated. After 24 h the specimens were divided into four groups at random and prior to bonding of a dual cure resin composite button were treated as follows: Group 1, no treatment (control); Group 2, non-activated resin applied for 5 min, cleaned in acetone for 3 min; Group 3, as for Group 2, with silane reapplied; Group 4, as for group 3, but re-etched for 30 s before reapplication of silane. After bonding the specimens were stored in water at room temperature for 7 days. Shear bond strength data were as follows: Group 1, 18.6 +/- 1.6; Group 2, 15.9 +/- 1.7; Group 3, 16.7 +/- 2.6; Group 4, 15.3 +/- 3.0 MPa. Fractured surfaces examined, under light microscopy and scanning electron microscopy (SEM), showed cohesive failure within the porcelain in all cases. The reduction in mean bond strength after application of a try-in resin was significant in Groups 2 and 4 compared with the control (ANOVA P < 0.05). No other significant differences were measured. In conclusion a single reapplication of silane maintained the bond strength of resin to porcelain when final cementation was preceded by a try-in procedure and cleaning.

Acetone↗

The strength of Class II composite resin restorations as affected by preparation design.

This study evaluated the load, applied to the marginal ridge, required to produce failure in Class II posterior composite resin restorations with four different preparation designs. In group 1, the preparation had an extension through the occlusal groove. The other three groups employed a proximal box-only (slot) preparation. Group 2 preparations had facial and lingual retention grooves that extended from the gingival floor to the occlusal surface; group 3 preparations were slots without grooves; and group 4 preparations were slots without grooves and with unsupported proximal enamel. After the restorations were thermocycled, their marginal ridges were flattened and loaded to failure. Mean (SD) failure loads were 438 (73) N in group 1; 383 (52) N in group 2; 297 (72) N in group 3; and 281 (63) N in group 4. Mean failure loads of groups 1 and 2 were not significantly different from each other but were significantly greater than failure loads for groups 3 and 4. Mean failure loads of groups 3 and 4 were not significantly different.

Analysis of Variance↗